Zirconia fine ceramic Spray Nozzle

Alternative and trade names
Zirconia fine ceramic Spray Nozzle
Want to keep this datasheet? Save it now in your required format

Description

Zirconia ceramic Spray Nozzle and pipe are superior to other materials on chemistry corrosion proof, wear resistance and themostability and so on.Therefore, it is widely used in conditions metal or other materials not reach the requirements.

This material data has been provided by Zhengzhou Sky Universe Trade Co.,LTD..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

6 g/cm³

Show Supplier Material materials with Density of 6 g/cm³

Grain size

0.5 μm

Show Supplier Material materials with Grain size of 0.5 μm

Maximum

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

200 GPa

Show Supplier Material materials with Elastic modulus of 200 GPa

Flexural strength

23.0 °C

950 MPa

Show Supplier Material materials with Flexural strength of 950 MPa

Minimum

Hardness, Vickers

23.0 °C

145 [-]

Show Supplier Material materials with Hardness, Vickers of 145 [-]

Minimum

Plane-Strain Fracture Toughnes

23.0 °C

9 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 9 MPa·√m

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

400.0 °C

9.6E-6 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9.6E-6 1/K

Mean value between 20°C and the mentioned temperature, for Zirconium ceramic structural parts

Thermal conductivity

23.0 °C

3 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 3 W/(m·K)

Minimum

Chemical properties

PropertyValueComment

Yttrium

5.2 %

Show Supplier Material materials with Yttrium of 5.2 %

Y₂O₃

Zirconium

94.8 %

Show Supplier Material materials with Zirconium of 94.8 %

ZrO₂

Technological properties

Property
Application areas

Nozzles