Zirconia Y-TZP (KZY1000)

Want to keep this datasheet? Save it now in your required format

Description

Nanoker produces ceramic components and tailor made products from KZY1000. The key benefits of Zirconia Y-TZP (KZY1000) are: High mechanical strength, very dense and non-porous, excellent wear resistance, excellent corrosion resistance, high impact resistance and toughness, low friction, biocompatibility.

This material data has been provided by Nanoker.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

6.02 g/cm³

Show Supplier Material materials with Density of 6.02 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

210 GPa

Show Supplier Material materials with Elastic modulus of 210 GPa

Flexural strength

23.0 °C

1000 MPa

Show Supplier Material materials with Flexural strength of 1000 MPa

Plane-Strain Fracture Toughnes

23.0 °C

6 MPa·√m

Show Supplier Material materials with Plane-Strain Fracture Toughnes of 6 MPa·√m

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

1000.0 °C

1.1E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.1E-5 1/K

Max service temperature

1000 °C

Show Supplier Material materials with Max service temperature of 1000 °C

no load

Thermal conductivity

23.0 °C

3 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 3 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

100000 Ω·m

Show Supplier Material materials with Electrical resistivity of 100000 Ω·m

Chemical properties

PropertyValueComment

Iron

7E-3 %

Show Supplier Material materials with Iron of 7E-3 %

as Fe₂O₃

Potassium

2E-3 %

Show Supplier Material materials with Potassium of 2E-3 %

as K₂O

Silicon

0.02 %

Show Supplier Material materials with Silicon of 0.02 %

as SiO₂

Sodium

5E-3 %

Show Supplier Material materials with Sodium of 5E-3 %

as Na₂O

Yttrium

5.19 %

Show Supplier Material materials with Yttrium of 5.19 %

as Y₂O₃

Zirconium

94 %

Show Supplier Material materials with Zirconium of 94 %

as ZrO₂

Technological properties

Property
Application areas

Typical application areas include: Medicine (implants), pump & compressor industry