General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Durchmesser |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Dureza Brinell of 120 - 150 [-] |
Dureza Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Dureza Vickers of 125 - 155 [-] |
Elongación | 20.0 °C | 20 % Show Material materials with Elongación of 20 % |
Límite elástico Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Límite elástico Rp 0,2 of 250 MPa |
Resistencia a la tracción | 20.0 °C | 500 MPa Show Material materials with Resistencia a la tracción of 500 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 6.3 - 7.6 % Show Material materials with Aluminio of 6.3 - 7.6 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.2 - 0.3 % Show Material materials with Hierro of 0.2 - 0.3 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Otro | Rest Cu, total 0.2 |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 1.5 - 2.2 % Show Material materials with Silicona of 1.5 - 2.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |