Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % |
Límite elástico | 23.0 °C | 400 MPa Show Supplier Material materials with Límite elástico of 400 MPa |
Resistencia a la tracción | 23.0 °C | 600 - 950 MPa Show Supplier Material materials with Resistencia a la tracción of 600 - 950 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.15 - 0.35 % Show Supplier Material materials with Azufre of 0.15 - 0.35 % |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % |
Cromo | 17 - 19 % Show Supplier Material materials with Cromo of 17 - 19 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Nitrógeno | 0.11 % Show Supplier Material materials with Nitrógeno of 0.11 % |
Níquel | 8 - 10 % Show Supplier Material materials with Níquel of 8 - 10 % |
Otro | 1 % Show Supplier Material materials with Otro of 1 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Precison components |