General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.78 g/cm³ Show Supplier Material materials with Densidad of 2.78 g/cm³ |
Rugosidad superficial | 0.4 μm Show Supplier Material materials with Rugosidad superficial of 0.4 μm |
Medidas
Property | Value |
---|---|
Espesor | 10 - 600 mm Show Supplier Material materials with Espesor of 10 - 600 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 130 - 135 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 130 - 135 [-] |
Elongación A50 | 23.0 °C | 1.5 - 8 % Show Supplier Material materials with Elongación A50 of 1.5 - 8 % |
Límite elástico | 23.0 °C | 290 - 310 MPa Show Supplier Material materials with Límite elástico of 290 - 310 MPa |
Módulo elástico | 23.0 °C | 72 GPa Show Supplier Material materials with Módulo elástico of 72 GPa |
Resistencia a la tracción | 23.0 °C | 325 - 360 MPa Show Supplier Material materials with Resistencia a la tracción of 325 - 360 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 2.37E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.37E-5 1/K | Mean values between 20°C and the mentioned temperature |
Conductividad térmica | 23.0 °C | 150 W/(m·K) Show Supplier Material materials with Conductividad térmica of 150 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.90E+7 - 2.30E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Technological properties
Property | ||
---|---|---|
Anodizing | good | |
Application areas | Tool making, mould making and model making; Injection moulds; Machine and fixture construction; Base plates, table tops and mounting plates | |
Corrosion properties | good | |
Dimensional stability | very good | |
General machinability | very good | |
Welding | WIG: good, Resistance welding: very good |