Medidas
Property | Value |
---|---|
Longitud | 6 - 101.6 mm Show Supplier Material materials with Longitud of 6 - 101.6 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -60.0 °C | 42 J Show Supplier Material materials with Charpy impact energy, V-notch of 42 J | Average of 3 tests |
Dureza Brinell | 23.0 °C | 187 - 321 [-] Show Supplier Material materials with Dureza Brinell of 187 - 321 [-] | |
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % | |
Energía de impacto Charpy, transversal | -60.0 °C | 21 J Show Supplier Material materials with Energía de impacto Charpy, transversal of 21 J | Average of 3 tests and V notched |
Estricción | 23.0 °C | 35 % Show Supplier Material materials with Estricción of 35 % | |
Límite elástico Rp 0,2 | 23.0 °C | 414 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 414 MPa | |
Resistencia a la tracción | 23.0 °C | 758 - 828 MPa Show Supplier Material materials with Resistencia a la tracción of 758 - 828 MPa | For thickness up to 250mm |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 1 % Show Supplier Material materials with Aluminio of 1 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | |
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | |
Cromo | 20 - 23 % Show Supplier Material materials with Cromo of 20 - 23 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | |
Hierro | 5 % Show Supplier Material materials with Hierro of 5 % | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | |
Molibdeno | 8 - 10 % Show Supplier Material materials with Molibdeno of 8 - 10 % | |
Niobio | 0.15 - 4.15 % Show Supplier Material materials with Niobio of 0.15 - 4.15 % | |
Níquel | 58 % Show Supplier Material materials with Níquel of 58 % | Balance |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | |
Titanio | 0.4 % Show Supplier Material materials with Titanio of 0.4 % |