Property | Value | Comment |
---|---|---|
Tamaño de grano | 2 μm Show Supplier Material materials with Tamaño de grano of 2 μm | Maximum, ASTM E112 |
Medidas
Property | Value |
---|---|
Longitud | 12.7 - 103.6 mm Show Supplier Material materials with Longitud of 12.7 - 103.6 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -60.0 °C | 68 J Show Supplier Material materials with Charpy impact energy, V-notch of 68 J | Average |
Dureza Brinell (HBW) | 23.0 °C | 298 - 363 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 298 - 363 [-] | |
Dureza Rockwell C | 23.0 °C | 32 - 40 [-] Show Supplier Material materials with Dureza Rockwell C of 32 - 40 [-] | |
Elongación | 23.0 °C | 20 % Show Supplier Material materials with Elongación of 20 % | |
Energía de impacto Charpy, transversal | -60.0 °C | 47 J Show Supplier Material materials with Energía de impacto Charpy, transversal of 47 J | Single value |
Estricción | 23.0 °C | 35 % Show Supplier Material materials with Estricción of 35 % | |
Límite elástico Rp 0,2 | 23.0 °C | 120 - 145 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 120 - 145 MPa | |
Resistencia a la tracción | 23.0 °C | 1034 MPa Show Supplier Material materials with Resistencia a la tracción of 1034 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.4 - 0.6 % Show Supplier Material materials with Aluminio of 0.4 - 0.6 % | ||
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | ||
Bismuto | 5E-5 % Show Supplier Material materials with Bismuto of 5E-5 % | ||
Boro | 6E-3 % Show Supplier Material materials with Boro of 6E-3 % | ||
Calcio | 3E-3 % Show Supplier Material materials with Calcio of 3E-3 % | ||
Carbono | 0.045 % Show Supplier Material materials with Carbono of 0.045 % | ||
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | ||
Cobre | 0.23 % Show Supplier Material materials with Cobre of 0.23 % | ||
Cromo | 17 - 21 % Show Supplier Material materials with Cromo of 17 - 21 % | ||
Fósforo | 0.01 % Show Supplier Material materials with Fósforo of 0.01 % | ||
Hierro | Balance | ||
Magnesio | 6E-3 % Show Supplier Material materials with Magnesio of 6E-3 % | ||
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % | ||
Molibdeno | 2.8 - 3.3 % Show Supplier Material materials with Molibdeno of 2.8 - 3.3 % | ||
Níquel | 55 % Show Supplier Material materials with Níquel of 55 % | ||
Otro | 4.78 - 5.2 % Show Supplier Material materials with Otro of 4.78 - 5.2 % | Cb+Ta | |
Plomo | 1E-3 % Show Supplier Material materials with Plomo of 1E-3 % | ||
Selenio | 5E-5 % Show Supplier Material materials with Selenio of 5E-5 % | ||
Silicona | 0.35 % Show Supplier Material materials with Silicona of 0.35 % | ||
Titanio | 0.8 - 1.15 % Show Supplier Material materials with Titanio of 0.8 - 1.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Ideal applicationsfor Alloy 718 are in oil tools, such as gate valves, choke stems, etc., and high strength applicationssuch as fasteners and turbines. |