Mecánica
Property | Temperature | Value | |
---|---|---|---|
Dureza Brinell | 23.0 °C | 290 [-] Show Supplier Material materials with Dureza Brinell of 290 [-] | |
Elongación | 23.0 °C | 23 % Show Supplier Material materials with Elongación of 23 % | |
Límite elástico Rp 0,2 | 23.0 °C | 530 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 530 MPa | |
Resistencia a la tracción | 23.0 °C | 730 - 930 MPa Show Supplier Material materials with Resistencia a la tracción of 730 - 930 MPa | |
Charpy impact energy, V-notch | 100 |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 3 - 4.5 % Show Supplier Material materials with Molibdeno of 3 - 4.5 % |
Nitrógeno | 0.24 - 0.35 % Show Supplier Material materials with Nitrógeno of 0.24 - 0.35 % |
Níquel | 6 - 8 % Show Supplier Material materials with Níquel of 6 - 8 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | F53 has excellent resistance to stress corrosion cracking in chloride bearing environments, excellent resistance to pitting , crevice and general corrosion. | |
Welding | Good |