General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.43 g/cm³ Show Supplier Material materials with Densidad of 8.43 g/cm³ | |
Tamaño de grano | 4 μm Show Supplier Material materials with Tamaño de grano of 4 μm | Maximum, ASTM E112 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 44 [-] Show Supplier Material materials with Dureza Rockwell C of 44 [-] | ASTM E18 |
Elongación | 23.0 °C | 8 % Show Supplier Material materials with Elongación of 8 % | ASTM E8, For 50.8mm diameter |
Estricción | 23.0 °C | 35 % Show Supplier Material materials with Estricción of 35 % | ASTM E8, For 50.8mm diameter |
Límite elástico Rp 0,2 | 23.0 °C | 230 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 230 MPa | ASTM E8, For 50.8mm diameter |
Resistencia a la tracción | 23.0 °C | 260 MPa Show Supplier Material materials with Resistencia a la tracción of 260 MPa | ASTM E8, For 50.8mm diameter |
Resistencia al cizallamiento | 23.0 °C | 1034 MPa Show Supplier Material materials with Resistencia al cizallamiento of 1034 MPa | For 25.4mm diameter |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % |
Boro | 0.15 % Show Supplier Material materials with Boro of 0.15 % |
Carbono | 0.025 % Show Supplier Material materials with Carbono of 0.025 % |
Cobalto | Balance |
Cromo | 19 - 21 % Show Supplier Material materials with Cromo of 19 - 21 % |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % |
Hierro | 1 % Show Supplier Material materials with Hierro of 1 % |
Manganeso | 0.15 % Show Supplier Material materials with Manganeso of 0.15 % |
Molibdeno | 9 - 10.5 % Show Supplier Material materials with Molibdeno of 9 - 10.5 % |
Níquel | 33 - 37 % Show Supplier Material materials with Níquel of 33 - 37 % |
Silicona | 0.15 % Show Supplier Material materials with Silicona of 0.15 % |
Titanio | 1 % Show Supplier Material materials with Titanio of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | The high strength variant of MP35N™ is used in a wide range of applications, in aerospace particularly for fasteners and airframe components. Elsewhere MP35N is used in motor sports, medical etc. for fasteners, springs, non-magnetic electrical components, instrument parts, valve components, high pressure door fittings, actuators, seals, shafts and other components. | |
Corrosion properties | This material has generally excellent corrosion resistance properties, including stress corrosion cracking (SCC) resistance for harsh environments as well as resists attack from mineral acids (nitric, hydrochloric and sulphur). The material also has exceptional resistance to crevice and stress corrosion cracking in hostile environments. |