Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 226 [-] Show Supplier Material materials with Dureza Brinell of 226 [-] |
Dureza Rockwell C | 23.0 °C | 20 [-] Show Supplier Material materials with Dureza Rockwell C of 20 [-] |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 555 - 621 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 555 - 621 MPa |
Resistencia a la tracción | 23.0 °C | 759 - 770 MPa Show Supplier Material materials with Resistencia a la tracción of 759 - 770 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 2 - 4 % Show Supplier Material materials with Aluminio of 2 - 4 % |
Cobre | Balance |
Cromo | 0.3 % Show Supplier Material materials with Cromo of 0.3 % |
Estaño | 0.3 % Show Supplier Material materials with Estaño of 0.3 % |
Hierro | 0.5 - 2.5 % Show Supplier Material materials with Hierro of 0.5 - 2.5 % |
Manganeso | 0.1 - 1 % Show Supplier Material materials with Manganeso of 0.1 - 1 % |
Níquel | 13 - 14 % Show Supplier Material materials with Níquel of 13 - 14 % |
Plomo | 0.3 % Show Supplier Material materials with Plomo of 0.3 % |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Zinc | 0.5 % Show Supplier Material materials with Zinc of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Bolt | |
Corrosion properties | Used where stress corrosion in ammonia / amine & sulphide environments is an issue. |