General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.43 g/cm³ Show Supplier Material materials with Densidad of 8.43 g/cm³ | |
Tamaño de grano | 4 μm Show Supplier Material materials with Tamaño de grano of 4 μm | Maximum, ASTM E112 |
Medidas
Property | Value |
---|---|
Longitud | 12.7 - 76.2 mm Show Supplier Material materials with Longitud of 12.7 - 76.2 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 51 [-] Show Supplier Material materials with Dureza Rockwell C of 51 [-] | |
Elongación | 23.0 °C | 10 % Show Supplier Material materials with Elongación of 10 % | ASTM E8, For 50.8mm diameter |
Estricción | 23.0 °C | 40 % Show Supplier Material materials with Estricción of 40 % | ASTM E8, For 50.8mm diameter |
Límite elástico Rp 0,2 | 23.0 °C | 180 - 210 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 180 - 210 MPa | ASTM E8, Depending on the aging, for 50.8mm diameter |
Resistencia a la tracción | 23.0 °C | 190 - 220 MPa Show Supplier Material materials with Resistencia a la tracción of 190 - 220 MPa | ASTM E8, Depending on the aging, for 50.8mm diameter |
Resistencia al cizallamiento | 23.0 °C | 1034 MPa Show Supplier Material materials with Resistencia al cizallamiento of 1034 MPa | For 25.4mm diameter |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % |
Boro | 0.15 % Show Supplier Material materials with Boro of 0.15 % |
Carbono | 0.025 % Show Supplier Material materials with Carbono of 0.025 % |
Cobalto | Balance |
Cromo | 19 - 21 % Show Supplier Material materials with Cromo of 19 - 21 % |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % |
Hierro | 1 % Show Supplier Material materials with Hierro of 1 % |
Manganeso | 0.15 % Show Supplier Material materials with Manganeso of 0.15 % |
Molibdeno | 9 - 10.5 % Show Supplier Material materials with Molibdeno of 9 - 10.5 % |
Níquel | 33 - 37 % Show Supplier Material materials with Níquel of 33 - 37 % |
Silicona | 0.15 % Show Supplier Material materials with Silicona of 0.15 % |
Titanio | 1 % Show Supplier Material materials with Titanio of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | NACE material is ideally suited for oil field equipment such as fasteners, springs, non-magnetic electrical components, instrument parts, valve components, high pressure door fittings, actuators, seals, shafts and other components. | |
Corrosion properties | MP35N in its NACE variant offers exceptional stress corrosion cracking (SCC) resistance for harsh environments such as hydrogen sulphide, salt water and other chloride environments, as well as resists attack from mineral acids (nitric, hydrochloric and sulphur). The material has exceptional resistance to crevice and stress corrosion cracking in sea water and other hostile environments. | |
Processing methods | Melting: MP35N™ is produced by vacuum induction melting followed by VAC-ARC remelting to provide exceptional control of chemistry and ingot solidification. |