General
Property | Value | Comment |
---|---|---|
Tamaño de grano | 5 μm Show Supplier Material materials with Tamaño de grano of 5 μm | Maximum, ASTM E112 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 27 - 40 J Show Supplier Material materials with Charpy impact energy, V-notch of 27 - 40 J | Depending on the Thickness |
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | |
Energía de impacto Izod | 23.0 °C | 27 J Show Supplier Material materials with Energía de impacto Izod of 27 J | |
Estricción | 23.0 °C | 50 % Show Supplier Material materials with Estricción of 50 % | |
Límite elástico Rp 0,2 | 24.0 °C | 660 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 660 MPa | |
100.0 °C | 624 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 624 MPa | ||
150.0 °C | 603 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 603 MPa | ||
200.0 °C | 595 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 595 MPa | ||
250.0 °C | 581 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 581 MPa | ||
300.0 °C | 573 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 573 MPa | ||
350.0 °C | 559 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 559 MPa | ||
400.0 °C | 537 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 537 MPa | ||
450.0 °C | 508 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 508 MPa | ||
500.0 °C | 464 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 464 MPa | ||
600.0 °C | 406 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 406 MPa | ||
Resistencia a la fluencia | 450.0 °C | 520 MPa Show Supplier Material materials with Resistencia a la fluencia of 520 MPa | For 10000 hours |
500.0 °C | 384 MPa Show Supplier Material materials with Resistencia a la fluencia of 384 MPa | For 10000 hours | |
550.0 °C | 261 MPa Show Supplier Material materials with Resistencia a la fluencia of 261 MPa | For 10000 hours | |
600.0 °C | 127 MPa Show Supplier Material materials with Resistencia a la fluencia of 127 MPa | For 10000 hours | |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.015 - 0.08 % Show Supplier Material materials with Aluminio of 0.015 - 0.08 % | ||
Arsénico | 0.02 % Show Supplier Material materials with Arsénico of 0.02 % | ||
Azufre | 0.08 % Show Supplier Material materials with Azufre of 0.08 % | ||
Boro | 0.001 - 0.01 % Show Supplier Material materials with Boro of 0.001 - 0.01 % | ||
Carbono | 0.17 - 0.23 % Show Supplier Material materials with Carbono of 0.17 - 0.23 % | ||
Cobre | 0.2 % Show Supplier Material materials with Cobre of 0.2 % | ||
Cromo | 0.9 - 1.2 % Show Supplier Material materials with Cromo of 0.9 - 1.2 % | ||
Estaño | 0.02 % Show Supplier Material materials with Estaño of 0.02 % | ||
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | ||
Hierro | Balance | ||
Manganeso | 0.35 - 0.75 % Show Supplier Material materials with Manganeso of 0.35 - 0.75 % | ||
Molibdeno | 0.9 - 1.1 % Show Supplier Material materials with Molibdeno of 0.9 - 1.1 % | ||
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % | ||
Otro | 0.1 % Show Supplier Material materials with Otro of 0.1 % | P+2.43As+3.57Sn+8.16Sb+0.13Cu | |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | ||
Titanio | 0.07 - 0.15 % Show Supplier Material materials with Titanio of 0.07 - 0.15 % | ||
Vanadio | 0.6 - 0.8 % Show Supplier Material materials with Vanadio of 0.6 - 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Fasteners with specified elevated and/or low temperature properties. |