Medidas
Property | Value |
---|---|
Longitud | 12.7 - 127 mm Show Supplier Material materials with Longitud of 12.7 - 127 mm |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 248 - 321 [-] Show Supplier Material materials with Dureza Brinell of 248 - 321 [-] | |
Dureza Rockwell C | 23.0 °C | 29 - 35 [-] Show Supplier Material materials with Dureza Rockwell C of 29 - 35 [-] | |
Elongación | 23.0 °C | 15 % Show Supplier Material materials with Elongación of 15 % | |
Estricción | 23.0 °C | 18 % Show Supplier Material materials with Estricción of 18 % | |
Límite elástico Rp 0,2 | 23.0 °C | 725 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 725 MPa | |
Resistencia a la fluencia | 650.0 °C | 385 MPa Show Supplier Material materials with Resistencia a la fluencia of 385 MPa | For 100 hours resulting in 5% elongation |
Resistencia a la tracción | 23.0 °C | 895 MPa Show Supplier Material materials with Resistencia a la tracción of 895 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.3 - 0.4 % Show Supplier Material materials with Aluminio of 0.3 - 0.4 % |
Azufre | 0.025 - 0.035 % Show Supplier Material materials with Azufre of 0.025 - 0.035 % |
Boro | 0.0001 - 0.01 % Show Supplier Material materials with Boro of 0.0001 - 0.01 % |
Carbono | 0.07 - 0.09 % Show Supplier Material materials with Carbono of 0.07 - 0.09 % |
Cromo | 13.5 - 16 % Show Supplier Material materials with Cromo of 13.5 - 16 % |
Fósforo | 0.04 - 0.05 % Show Supplier Material materials with Fósforo of 0.04 - 0.05 % |
Hierro | Balance |
Manganeso | 1.96 - 2.04 % Show Supplier Material materials with Manganeso of 1.96 - 2.04 % |
Molibdeno | 1 - 1.5 % Show Supplier Material materials with Molibdeno of 1 - 1.5 % |
Níquel | 24 - 27 % Show Supplier Material materials with Níquel of 24 - 27 % |
Silicona | 0.95 - 1.05 % Show Supplier Material materials with Silicona of 0.95 - 1.05 % |
Titanio | 1.9 - 2.35 % Show Supplier Material materials with Titanio of 1.9 - 2.35 % |
Vanadio | 0.1 - 0.5 % Show Supplier Material materials with Vanadio of 0.1 - 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Bolts, fasteners, turbines, critical framesin high stress / heat applications, castings and fasteners. |