General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.87 g/cm³ Show Supplier Material materials with Densidad of 8.87 g/cm³ |
Medidas
Property | Value |
---|---|
Diámetro | 10 - 250 mm Show Supplier Material materials with Diámetro of 10 - 250 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 325 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 325 [-] |
Dureza Rockwell C | 23.0 °C | 35 [-] Show Supplier Material materials with Dureza Rockwell C of 35 [-] |
Elongación | 23.0 °C | 40 % Show Supplier Material materials with Elongación of 40 % |
Límite elástico Rp 0,2 | 23.0 °C | 283 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 283 MPa |
Resistencia a la tracción | 23.0 °C | 690 MPa Show Supplier Material materials with Resistencia a la tracción of 690 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % |
Cobalto | 2.5 % Show Supplier Material materials with Cobalto of 2.5 % |
Cromo | 14.5 - 16.5 % Show Supplier Material materials with Cromo of 14.5 - 16.5 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | 4 - 7 % Show Supplier Material materials with Hierro of 4 - 7 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 15 - 17 % Show Supplier Material materials with Molibdeno of 15 - 17 % |
Níquel | Balance |
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % |
Vanadio | 0.35 % Show Supplier Material materials with Vanadio of 0.35 % |
Wolframio | 3 - 4 % Show Supplier Material materials with Wolframio of 3 - 4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Alloy C276 can be used in the most severe environments such as chemical and petrochemical processing involving bleach, pollution control, pulp and paper production, industrial and municipal waste treatment, pharmaceutical and food processing equipment, and process plant involved in the recovery of sour natural gas. Alloy C276 is ideal for use in evaporators, heat exchangers, sulphuric acid filters and reactors, and process plant handling acid catalysts. | |
Corrosion properties | C276 is resistant to pitting, stress corrosion cracking, and crevice corrosion in a wide range of chemical environments, particularly in chloride gas, hypochlorite and chlorine dioxide solutions. Meanwhile the chromium content adds resistance to oxidizing media, such as ferric and cupric chlorides. To complete the overall corrosion resisting properties, tungsten is present to provide additional general resistance in a wide range of severe environments. | |
Welding | Welding properties are good, with the low carbon content minimizing carbide / grain boundary precipitation during welding to maintain corrosion resistance in the welded finished condition. |