Medidas
Property | Value |
---|---|
Diámetro | 12.7 - 250 mm Show Supplier Material materials with Diámetro of 12.7 - 250 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 23.0 °C | 310 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 310 MPa |
Módulo elástico | 23.0 °C | 180 GPa Show Supplier Material materials with Módulo elástico of 180 GPa |
Resistencia a la tracción | 23.0 °C | 550 MPa Show Supplier Material materials with Resistencia a la tracción of 550 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Supplier Material materials with Aluminio of 0.5 % |
Azufre | 0.24 % Show Supplier Material materials with Azufre of 0.24 % |
Carbono | 0.3 % Show Supplier Material materials with Carbono of 0.3 % |
Cobre | 28 - 34 % Show Supplier Material materials with Cobre of 28 - 34 % |
Hierro | 2.5 % Show Supplier Material materials with Hierro of 2.5 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Níquel | 63 - 70 % Show Supplier Material materials with Níquel of 63 - 70 % |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Valves, Fasteners and Marine engineering, Chemical and hydrocarbon processing equipment, Pumps, Propeller shafts, Oil and fresh water tanks, Fittings, Heat exchangers |