Mecánica
Property | Temperature | Value | |
---|---|---|---|
Dureza Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Dureza Brinell of 270 [-] | |
Elongación | 23.0 °C | 25 % Show Supplier Material materials with Elongación of 25 % | |
Estricción | 23.0 °C | 45 % Show Supplier Material materials with Estricción of 45 % | |
Límite elástico Rp 0,2 | 23.0 °C | 485 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 485 MPa | |
Resistencia a la tracción | 23.0 °C | 655 - 880 MPa Show Supplier Material materials with Resistencia a la tracción of 655 - 880 MPa | |
Charpy impact energy, V-notch | 45;-46,100;25 |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % |
Cromo | 21 - 23 % Show Supplier Material materials with Cromo of 21 - 23 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 2.5 - 3.5 % Show Supplier Material materials with Molibdeno of 2.5 - 3.5 % |
Nitrógeno | 0.1 - 0.22 % Show Supplier Material materials with Nitrógeno of 0.1 - 0.22 % |
Níquel | 4.5 - 6.5 % Show Supplier Material materials with Níquel of 4.5 - 6.5 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications in the power generation and oil & gas industry include pumps, valves, pipework, flanges, bolting, connectors & manifolds. | |
Corrosion properties | F51 resists chloride environments and sulphide stress corrosion. Corrossion Test to ASTM G48 Method A 25°C for 24 hours |