Medidas
Property | Value |
---|---|
Ancho | 900 - 1100 mm Show Supplier Material materials with Ancho of 900 - 1100 mm |
Espesor | 200 - 500 mm Show Supplier Material materials with Espesor of 200 - 500 mm |
Mecánica
Property | Value |
---|---|
Dureza Rockwell C | 38 - 42 [-] Show Supplier Material materials with Dureza Rockwell C of 38 - 42 [-] |
Resistencia a la tracción | 1190 - 1320 MPa Show Supplier Material materials with Resistencia a la tracción of 1190 - 1320 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.04e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.04e-05 1/K | for 20°C to the mentioned temperature |
150 °C | 1.06e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.06e-05 1/K | for 20°C to the mentioned temperature | |
200 °C | 1.09e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.09e-05 1/K | for 20°C to the mentioned temperature | |
250 °C | 1.11e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.14e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.14e-05 1/K | for 20°C to the mentioned temperature | |
350 °C | 1.15e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.15e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.17e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.17e-05 1/K | for 20°C to the mentioned temperature | |
450 °C | 1.19e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.19e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 23 °C | 16.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 16.8 W/(m·K) | |
150 °C | 20.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 20.1 W/(m·K) | ||
300 °C | 22.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 22.1 W/(m·K) | ||
350 °C | 22.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 22.8 W/(m·K) | ||
400 °C | 23.3 W/(m·K) Show Supplier Material materials with Conductividad térmica of 23.3 W/(m·K) | ||
500 °C | 24.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 24.1 W/(m·K) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Carbono | 0.05 % Show Supplier Material materials with Carbono of 0.05 % | ||
Cromo | 15 % Show Supplier Material materials with Cromo of 15 % | ||
Hierro | Balance | ||
Manganeso | 0.3 % Show Supplier Material materials with Manganeso of 0.3 % | ||
Níquel | 4.5 % Show Supplier Material materials with Níquel of 4.5 % | ||
Otro | 3.5 % Show Supplier Material materials with Otro of 3.5 % | Cu + Nb | |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Technological properties
Property | ||
---|---|---|
Application areas | High polished tools and moulds for processing of high corrosive plastics, tools for plastic extrusion. | |
Heat Treatment | Formadur PH X Superclean usually is supplied in precipitation-hardened condition with a hardness of 40 HRC. |