Coeficiente de dilatación térmica: 1.2E-5 1/K

Quick Comparison

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 12CrMoV12-10 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoSi5-5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Molybdenum Steel

EN 10028-2 Grade 13CrMoV9-10 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Medium Carbon Steel

ISO 683-1 Grade C45E quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S550QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S500QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620Q quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S620QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Chromium Steel

ISO 683-3 Grade 16MnCr5 normalized or normalized formed (+N)

Suministrada por:

1 proveedor Matmatch

Polietileno tereftalato (PET)

Rynite® FR515 NC010

Polyamide 66 (PA66)

TECACOMP PA66 TRM XS black 4074

Suministrada por:

Ensinger GmbH

Compuesto de matriz de polímero termoendurecible

Epoxy NP130 - Sheet

Suministrada por:

Norplex-Micarta

Chromium Molybdenum Steel

ASTM A542 Type E Class 4 Quenched and Tempered

Suministrada por:

1 proveedor Matmatch

Polyamide 66 (PA66)

Zytel® FR50 BK505
Página 1 de 152