Medidas
Property | Value |
---|---|
Diámetro | 232 - 363 mm Show Supplier Material materials with Diámetro of 232 - 363 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 230 [-] Show Supplier Material materials with Dureza Brinell of 230 [-] | soft annealed |
Dureza Rockwell C | 42 - 52 [-] Show Supplier Material materials with Dureza Rockwell C of 42 - 52 [-] | |
Resistencia a la tracción | 1320 - 1775 MPa Show Supplier Material materials with Resistencia a la tracción of 1320 - 1775 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.15e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.15e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.23e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.23e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.26e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.26e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.29e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.29e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.32e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.32e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 28.36 W/(m·K) Show Supplier Material materials with Conductividad térmica of 28.36 W/(m·K) | |
100 °C | 29.3 W/(m·K) Show Supplier Material materials with Conductividad térmica of 29.3 W/(m·K) | ||
200 °C | 30.9 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30.9 W/(m·K) | ||
300 °C | 31 W/(m·K) Show Supplier Material materials with Conductividad térmica of 31 W/(m·K) | ||
400 °C | 30.7 W/(m·K) Show Supplier Material materials with Conductividad térmica of 30.7 W/(m·K) | ||
500 °C | 29.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 29.5 W/(m·K) | ||
600 °C | 27.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 27.8 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.35 % Show Supplier Material materials with Carbono of 0.35 % |
Cromo | 5 % Show Supplier Material materials with Cromo of 5 % |
Hierro | Balance |
Manganeso | 0.3 % Show Supplier Material materials with Manganeso of 0.3 % |
Otro | Plus additions |
Silicona | 0.3 % Show Supplier Material materials with Silicona of 0.3 % |
Vanadio | 0.8 % Show Supplier Material materials with Vanadio of 0.8 % |
Technological properties
Property | ||
---|---|---|
Application areas | Universally usable for highly stressed tools and highest temperatures, casting dies for light metal processing (especially for complex tools), extrusion dies for light and heavy metal processing (especially for complexly formed profiles), dies and inserts | |
Heat Treatment | Soft annealing: 750-800°C (Cooling in furnace) - Hardening: 1020-1040°C and quenching in air, oil or hot bath T=500-550°C |