Medidas
Property | Value |
---|---|
Ancho | 800 - 950 mm Show Supplier Material materials with Ancho of 800 - 950 mm |
Espesor | 300 - 420 mm Show Supplier Material materials with Espesor of 300 - 420 mm |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Brinell | 220 [-] Show Supplier Material materials with Dureza Brinell of 220 [-] | soft annealed |
Dureza Rockwell C | 40 - 52 [-] Show Supplier Material materials with Dureza Rockwell C of 40 - 52 [-] | |
Resistencia a la tracción | 1255 - 1775 MPa Show Supplier Material materials with Resistencia a la tracción of 1255 - 1775 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.2e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.2e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.23e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.23e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.27e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.27e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.31e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.31e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 100 °C | 44 W/(m·K) Show Supplier Material materials with Conductividad térmica of 44 W/(m·K) | |
200 °C | 43 W/(m·K) Show Supplier Material materials with Conductividad térmica of 43 W/(m·K) | ||
300 °C | 41 W/(m·K) Show Supplier Material materials with Conductividad térmica of 41 W/(m·K) | ||
400 °C | 39 W/(m·K) Show Supplier Material materials with Conductividad térmica of 39 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.45 % Show Supplier Material materials with Carbono of 0.45 % |
Cromo | 1.5 % Show Supplier Material materials with Cromo of 1.5 % |
Hierro | Balance |
Manganeso | 0.9 % Show Supplier Material materials with Manganeso of 0.9 % |
Níquel | 0.9 % Show Supplier Material materials with Níquel of 0.9 % |
Vanadio | 1.5 % Show Supplier Material materials with Vanadio of 1.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Special steel for press hardening, also useable for small plastic injection moulds | |
Heat Treatment | Soft annealing: 860°C (Cooling in furnace) - Hardening: 1080-1120°C and quenching in air, oil or hot bath T=500-550°C |