Property | Value | Comment |
---|---|---|
Dureza Brinell | 340 [-] Show Supplier Material materials with Dureza Brinell of 340 [-] | soft annealed |
Dureza Rockwell C | 51 - 55 [-] Show Supplier Material materials with Dureza Rockwell C of 51 - 55 [-] | |
Resistencia a la tracción | 1740 - 1995 MPa Show Supplier Material materials with Resistencia a la tracción of 1740 - 1995 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 100 °C | 1.03e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.03e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.1e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.1e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.12e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.12e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.15e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.15e-05 1/K | for 20°C to the mentioned temperature | |
500 °C | 1.18e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.18e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.16e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.16e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 14.2 W/(m·K) Show Supplier Material materials with Conductividad térmica of 14.2 W/(m·K) | |
350 °C | 18.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 18.5 W/(m·K) | ||
700 °C | 22.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 22.5 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % |
Cobalto | 10 % Show Supplier Material materials with Cobalto of 10 % |
Hierro | Balance |
Molibdeno | 5 % Show Supplier Material materials with Molibdeno of 5 % |
Níquel | 18 % Show Supplier Material materials with Níquel of 18 % |
Titanio | 1 % Show Supplier Material materials with Titanio of 1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Casings for cold extrusion tools, casting dies, plastic moulds | |
Heat Treatment | Soft annealing: 820-850°C (Cooling in furnace) - Percipitation temperature: 490°C, 4hr in air |