Conductividad térmica: 22.5 W/(m·K)

Quick Comparison

Medium Carbon Steel

EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Acero inoxidable martensítico

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Suministrada por:

1 proveedor Matmatch

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Suministrada por:

1 proveedor Matmatch

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Wrought Copper Nickel Silver Grade

ARCAP® AP4 O - CuNi44Mn0.8

Suministrada por:

Lebronze Alloys

Wrought Copper Nickel Silver Grade

ARCAP® AP4 H11 - CuNi44Mn0.8

Suministrada por:

Lebronze Alloys

Wrought Copper Nickel Silver Grade

ARCAP® AP4 H12 - CuNi44Mn0.8

Suministrada por:

Lebronze Alloys

Wrought Copper Nickel Silver Grade

ARCAP® AP4 H15 - CuNi44Mn0.8

Suministrada por:

Lebronze Alloys