General
Property | Value |
---|---|
Densidad | 7.2 g/cm³ Show Supplier Material materials with Densidad of 7.2 g/cm³ |
Mecánica
Property | Value |
---|---|
Dureza Rockwell C | 60 - 63 [-] Show Supplier Material materials with Dureza Rockwell C of 60 - 63 [-] |
Módulo elástico | 220 GPa Show Supplier Material materials with Módulo elástico of 220 GPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Supplier Material materials with Azufre of 0.05 % |
Carbono | 2.9 % Show Supplier Material materials with Carbono of 2.9 % |
Cromo | 5.3 % Show Supplier Material materials with Cromo of 5.3 % |
Hierro | Balance |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % |
Molibdeno | 1.3 % Show Supplier Material materials with Molibdeno of 1.3 % |
Silicona | 0.9 % Show Supplier Material materials with Silicona of 0.9 % |
Vanadio | 12 % Show Supplier Material materials with Vanadio of 12 % |
Technological properties
Property | ||
---|---|---|
Application areas | Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes, screw conveyors |