Wrought Copper Bronze Aluminium Bronze
AMPCO® 21 Extruded and drawn rounds and rectangular barsSuministrada por:
AMPCO METALGrey Cast Iron
EN 1561 Grade GJL-250 cast conditionDuctile (Nodular) Cast Iron
EN 1563 Grade GJS-600-3 heat treatment by manufacturer or by agreementDuctile (Nodular) Cast Iron
EN 1563 Grade GJS-700-2 heat treatment by manufacturer or by agreementDuctile (Nodular) Cast Iron
EN 1563 Grade GJS-800-2 heat treatment by manufacturer or by agreementMalleable Cast Iron
SAE J158 Grade M3210 AnnealedMalleable Cast Iron
SAE J158 Grade M4504 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5003 Air quenched and TemperedMalleable Cast Iron
SAE J158 Grade M5503 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M7002 Liquid quenched and TemperedMalleable Cast Iron
SAE J158 Grade M8501 Liquid quenched and TemperedMalleable Cast Iron
EN 1562 Grade GJMW-360-12 decarburized annealedUnclassified Zinc
DIN 17770 Grade ZnCuTiPolyamide 12 (PA12)
Polyamide 12 + Metal Powder (PA12+MED)Hierro fundido
EN 1562 Grade GJMB-350-10 not decarburized annealedHierro fundido
EN 1562 Grade GJMB-450-6 not decarburized annealed