General
Property | Value |
---|---|
Densidad | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Value |
---|---|
Dureza Rockwell C | 63 - 69 [-] Show Supplier Material materials with Dureza Rockwell C of 63 - 69 [-] |
Módulo elástico | 250 GPa Show Supplier Material materials with Módulo elástico of 250 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 420 J/(kg·K) Show Supplier Material materials with Calor específico of 420 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100 °C | 1.01e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.01e-05 1/K | for 20°C to the mentioned temperature |
200 °C | 1.03e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.03e-05 1/K | for 20°C to the mentioned temperature | |
300 °C | 1.06e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.06e-05 1/K | for 20°C to the mentioned temperature | |
400 °C | 1.08e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.08e-05 1/K | for 20°C to the mentioned temperature | |
600 °C | 1.11e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.11e-05 1/K | for 20°C to the mentioned temperature | |
Conductividad térmica | 20 °C | 22.5 W/(m·K) Show Supplier Material materials with Conductividad térmica of 22.5 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Carbono | 2.3 % Show Supplier Material materials with Carbono of 2.3 % |
Cobalto | 10.5 % Show Supplier Material materials with Cobalto of 10.5 % |
Cromo | 4.2 % Show Supplier Material materials with Cromo of 4.2 % |
Hierro | Balance |
Molibdeno | 7 % Show Supplier Material materials with Molibdeno of 7 % |
Vanadio | 6.5 % Show Supplier Material materials with Vanadio of 6.5 % |
Wolframio | 7 % Show Supplier Material materials with Wolframio of 7 % |
Technological properties
Property | ||
---|---|---|
Application areas | Heavy-duty cutting tools with very high requirements on red hardness and wear resistance |