General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.13 g/cm³ Show Supplier Material materials with Densidad of 1.13 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore A | 92 [-] Show Supplier Material materials with Dureza Shore A of 92 [-] | dry | ISO 868 | 3s |
Dureza Shore D | 33 [-] Show Supplier Material materials with Dureza Shore D of 33 [-] | dry | ISO 868 | 3s |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 0.05 GPa Show Supplier Material materials with Módulo elástico of 0.05 GPa | dry | ISO 527-1/-2 | |
Resistencia a la tracción | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 160 °C Show Supplier Material materials with Temperatura de fusión of 160 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -58.0 °C Show Supplier Material materials with Temperatura de transición del vidrio of -58.0 °C | dry | ASTM D5026/D7028 | DMTA (tan d) |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 33 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 33 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |