General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Elongación | 3.3 % Show Supplier Material materials with Elongación of 3.3 % | dry | ISO 527-1/-2 | |
5.6 % Show Supplier Material materials with Elongación of 5.6 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | conditioned | ISO 178 | |
260 MPa Show Supplier Material materials with Flexural yield strength of 260 MPa | dry | ISO 178 | ||
Módulo de flexión | 5.6 GPa Show Supplier Material materials with Módulo de flexión of 5.6 GPa | conditioned | ISO 178 | |
9.2 GPa Show Supplier Material materials with Módulo de flexión of 9.2 GPa | dry | ISO 178 | ||
Módulo elástico | 5.7 GPa Show Supplier Material materials with Módulo elástico of 5.7 GPa | conditioned | ISO 527-1/-2 | |
9.6 GPa Show Supplier Material materials with Módulo elástico of 9.6 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 110 MPa Show Supplier Material materials with Resistencia a la tracción of 110 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Resistencia a la tracción of 170 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry | ISO 179/1eA |
23 °C | 19 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 19 kJ/m² | conditioned | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 81 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 81 kJ/m² | dry | ISO 179/1eU |
23 °C | 92 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 92 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
7e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Temperatura de flexión bajo carga | 205 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 205 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 2e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+14 Ω/sq | conditioned | IEC 62631-3-2 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Contracción | 0.3 % Show Supplier Material materials with Contracción of 0.3 % | dry | ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Contracción of 1 % | dry | ISO 294-4 | Normal | ||
Velocidad de flujo del volumen derretido | 250 °C | 31 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 31 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |