General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 2.2 % Show Supplier Material materials with Absorción de agua of 2.2 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.36 g/cm³ Show Supplier Material materials with Densidad of 1.36 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|---|
Elongación | 2.9 % Show Supplier Material materials with Elongación of 2.9 % | dry | 1 mm | ISO 527-1/-2 | ||
3.2 % Show Supplier Material materials with Elongación of 3.2 % | dry | 1 mm | ISO 527-1/-2 | |||
3.4 % Show Supplier Material materials with Elongación of 3.4 % | conditioned | ISO 527-1/-2 | ||||
Flexural yield strength | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | conditioned | ISO 178 | |||
190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | ||||
Módulo de flexión | 5 GPa Show Supplier Material materials with Módulo de flexión of 5 GPa | conditioned | ISO 178 | |||
7.5 GPa Show Supplier Material materials with Módulo de flexión of 7.5 GPa | dry | ISO 178 | ||||
Módulo elástico | 5 GPa Show Supplier Material materials with Módulo elástico of 5 GPa | conditioned | ISO 527-1/-2 | |||
7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | dry | 1 mm | ISO 527-1/-2 | |||
7.5 GPa Show Supplier Material materials with Módulo elástico of 7.5 GPa | dry | 1 mm | ISO 527-1/-2 | |||
Resistencia a la tracción | 85 MPa Show Supplier Material materials with Resistencia a la tracción of 85 MPa | conditioned | ISO 527-1/-2 | |||
120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | 1 mm | ISO 527-1/-2 | |||
130 MPa Show Supplier Material materials with Resistencia a la tracción of 130 MPa | dry | 1 mm | ISO 527-1/-2 | at low thickness | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | conditioned | ISO 179/1eA | |||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 49 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 49 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 53 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 53 kJ/m² | conditioned | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 2.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6.5e-07 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | dry | UL746B | 0.2 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.2 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.2 mm | ||
Temperatura de flexión bajo carga | 285 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 285 °C | dry | ISO 75-1/-2 | 2 MPa | ||
Temperatura de fusión | 295 °C Show Supplier Material materials with Temperatura de fusión of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | 75 °C Show Supplier Material materials with Temperatura de transición del vidrio of 75 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 60250 | 1GHz |
3.6 [-] Show Supplier Material materials with Constante dieléctrica of 3.6 [-] | dry | IEC 60250 | 10GHz | |
3.7 [-] Show Supplier Material materials with Constante dieléctrica of 3.7 [-] | conditioned | IEC 60250 | 10GHz | |
3.75 [-] Show Supplier Material materials with Constante dieléctrica of 3.75 [-] | conditioned | IEC 60250 | 1GHz | |
Factor de disipación | 100 [-] Show Supplier Material materials with Factor de disipación of 100 [-] | dry | IEC 60250 | 1GHz |
100 [-] Show Supplier Material materials with Factor de disipación of 100 [-] | dry | IEC 60250 | 10GHz | |
180 [-] Show Supplier Material materials with Factor de disipación of 180 [-] | conditioned | IEC 60250 | 10GHz | |
210 [-] Show Supplier Material materials with Factor de disipación of 210 [-] | conditioned | IEC 60250 | 1GHz | |
Rigidez dieléctrica | 30 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 30 kV/mm | conditioned | IEC 60243-1 | |
33 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 33 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 7e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 7e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Volume resistivity | 4e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 4e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 | ||
Índice de seguimiento comparativo | 550 V Show Supplier Material materials with Índice de seguimiento comparativo of 550 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Reflow connectors (2) | |
Certifications | Yellow Card Available | |
Fillers | 20% Glass Fiber |