General
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Absorción de agua | 0.2 % Show Supplier Material materials with Absorción de agua of 0.2 % | dry | ISO 62 | at 23°C after 24h |
Densidad | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | dry | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore A | 98 [-] Show Supplier Material materials with Dureza Shore A of 98 [-] | dry | ISO 868 | 3s | |
98 [-] Show Supplier Material materials with Dureza Shore A of 98 [-] | dry | ISO 868 | 15s | ||
Dureza Shore D | 61 [-] Show Supplier Material materials with Dureza Shore D of 61 [-] | dry | ISO 868 | 15s | |
64 [-] Show Supplier Material materials with Dureza Shore D of 64 [-] | dry | ISO 868 | 3s | ||
Elongación | 300 % Show Supplier Material materials with Elongación of 300 % | dry | ISO 527-1/-2 | ||
460 % Show Supplier Material materials with Elongación of 460 % | dry | ISO 527-1/-2 | |||
530 % Show Supplier Material materials with Elongación of 530 % | dry | ISO 527-1/-2 | |||
Módulo elástico | 0.33 GPa Show Supplier Material materials with Módulo elástico of 0.33 GPa | dry | ISO 527-1/-2 | ||
Resistencia a desgarros | 171 kN/m Show Supplier Material materials with Resistencia a desgarros of 171 kN/m | dry | ISO 34-1; Method B | ||
187 kN/m Show Supplier Material materials with Resistencia a desgarros of 187 kN/m | dry | ISO 34-1; Method B | |||
Resistencia a la tracción | 34 MPa Show Supplier Material materials with Resistencia a la tracción of 34 MPa | dry | ISO 527-1/-2 | Normal | |
36 MPa Show Supplier Material materials with Resistencia a la tracción of 36 MPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 3.7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 3.7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 23 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 23 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 205 °C Show Supplier Material materials with Temperatura de fusión of 205 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 95 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 95 °C | dry | ISO 306 | 50°C/h 50N |
Eléctrico
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Constante dieléctrica | 4.3 [-] Show Supplier Material materials with Constante dieléctrica of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz |
Factor de disipación | 495 [-] Show Supplier Material materials with Factor de disipación of 495 [-] | dry | IEC 62631-2-1 | 1MHz |
Rigidez dieléctrica | 14.4 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 14.4 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 230 °C | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire and Cable Insulation | |
Certifications | Yellow Card Available |