General
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Densidad | 25 °C | 1.055 g/cm³ Show Supplier Material materials with Densidad of 1.055 g/cm³ | ISO 1183-1 |
Mecánica
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 15 % Show Supplier Material materials with Elongación of 15 % | ISO 527-1/2 | min. | 50 mm/min | |
Elongation at yield | 2.6 % Show Supplier Material materials with Elongation at yield of 2.6 % | ISO 527-1/2 | 50 mm/min | |
Flexural strain | 20 % Show Supplier Material materials with Flexural strain of 20 % | ISO 527-1/2 | 50 mm/min | |
Hardness, Ball Indentation | 106 MPa Show Supplier Material materials with Hardness, Ball Indentation of 106 MPa | ISO 2039-1 | ||
Límite elástico | 50.5 MPa Show Supplier Material materials with Límite elástico of 50.5 MPa | ISO 527-1/2 | 50 mm/min | |
Módulo de flexión | 2.6 GPa Show Supplier Material materials with Módulo de flexión of 2.6 GPa | ISO 527-1/2 | 2 mm/min | |
Módulo elástico | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | ISO 527-1/2 | 1 mm/min | |
Resistencia a la flexión | 75 MPa Show Supplier Material materials with Resistencia a la flexión of 75 MPa | ISO 178 | 2 mm/min | |
Resistencia a la tracción | 36.5 MPa Show Supplier Material materials with Resistencia a la tracción of 36.5 MPa | ISO 527-1/2 | 50 mm/min | |
Resistencia al choque, ensayo Charpy entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO 179-1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | ISO 179-1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 100 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² | ISO 179-1eU | |
23 °C | 124 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 124 kJ/m² | ISO 179-1eU | ||
Resistencia al choque, ensayo Izod entallado | -30 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 7 kJ/m² | ISO 180-1A | |
23 °C | 15 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 15 kJ/m² | ISO 180-1A |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 7.8e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.8e-05 1/K | ISO 11359-1/2 | 23 to 55°C | ||||
8.1e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.1e-05 1/K | ISO 11359-1/2 | 23 to 55°C, Transverse | |||||
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | IEC 60695-2-12 | 2.0 mm | ||||
Temperatura de flexión bajo carga | 94 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 94 °C | ISO 75-1/2 | 1.8 MPa | ||||
98 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 98 °C | ISO 75-1/2 | 0.45 MPa | |||||
Temperatura de reblandecimiento Vicat | 98 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 98 °C | ISO 306 | 50 N | 50°C/h | ||||
101 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 101 °C | ISO 306 | 50 N | 120°C/h | |||||
Inflamabilidad | At thickness 1.6 mm UL 94: HB |
Eléctrico
Property | Value | Frequency | Testing Standard |
---|---|---|---|
Constante dieléctrica | 2.82 [-] Show Supplier Material materials with Constante dieléctrica of 2.82 [-] | 1MHz | IEC 60250 |
3.04 [-] Show Supplier Material materials with Constante dieléctrica of 3.04 [-] | 100Hz | IEC 60250 | |
Factor de disipación | 0.0053 [-] Show Supplier Material materials with Factor de disipación of 0.0053 [-] | 100Hz | IEC 60250 |
0.0096 [-] Show Supplier Material materials with Factor de disipación of 0.0096 [-] | 1MHz | IEC 60250 | |
Surface resistivity | 2e+17 Ω/sq Show Supplier Material materials with Surface resistivity of 2e+17 Ω/sq | ||
Volume resistivity | 2e+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+16 Ω·cm | IEC 60093 |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Contracción | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | ISO 2577 | 150x105x3 | 500 bar |
0.5 % Show Supplier Material materials with Contracción of 0.5 % | ISO 2577 | 150x105x3 | 500 bar, Transverse | |
Velocidad de flujo del volumen derretido | 20 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 20 cm³/10min | ISO 1133 | 220°C/10Kg |
Technological properties
Property | ||
---|---|---|
Certifications | UL Certificate | |
Handling recommendations | Please see the Material Safety Data Sheet for relevant health & safety information. | |
Other | Control measurements in other places may issue different results due to influences of machinery, equipment, test method or storage conditions. | |
Processing methods | Injection molding-melt temperature: 240 ºC according to ISO 294 Injection molding-mold temperature: 70 ºC according to ISO 294 Injection molding-injection velocity: 240 mm/s according to ISO 294 |