General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Densidad of 2.7 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Standard stock sizes: 3000mm and 10-300mm in thickness |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 95 [-] | Test method: 2.5/62.5 |
Elongación A5 | 23.0 °C | 6 - 8 % Show Supplier Material materials with Elongación A5 of 6 - 8 % | |
Límite elástico Rp 0,2 | 23.0 °C | 200 - 260 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 200 - 260 MPa | |
Módulo elástico | 23.0 °C | 70 GPa Show Supplier Material materials with Módulo elástico of 70 GPa | |
Resistencia a la tracción | 23.0 °C | 270 - 310 MPa Show Supplier Material materials with Resistencia a la tracción of 270 - 310 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 896 J/(kg·K) Show Supplier Material materials with Calor específico of 896 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.34E-5 1/K |
Conductividad térmica | 23.0 °C | 170 - 220 W/(m·K) Show Supplier Material materials with Conductividad térmica of 170 - 220 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.40E+7 - 3.20E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.40E+7 - 3.20E+7 S/m |
Technological properties
Property | ||
---|---|---|
Processing history | Temper: T6, T651, T6511 |