General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.76 g/cm³ Show Supplier Material materials with Densidad of 2.76 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Standard stock sizes: 1520mm x 3020mm and 8-100mm in thickness, 1400mm x 3020mm and 110mm in thickness, 1200mm x 3020mm and 120mm in thickness, 1020mm x 3020mm and 130mm in thickness, 950mm x 3020mm and 140mm in thickness |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 167 - 170 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 167 - 170 [-] | Test method: 2.5/62.5 |
Elongación A50 | 23.0 °C | 6 - 9 % Show Supplier Material materials with Elongación A50 of 6 - 9 % | |
Límite elástico Rp 0,2 | 23.0 °C | 400 - 495 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 400 - 495 MPa | |
Módulo elástico | 23.0 °C | 72 GPa Show Supplier Material materials with Módulo elástico of 72 GPa | |
Resistencia a la tracción | 23.0 °C | 490 - 555 MPa Show Supplier Material materials with Resistencia a la tracción of 490 - 555 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 862 J/(kg·K) Show Supplier Material materials with Calor específico of 862 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.36E-5 1/K |
Conductividad térmica | 23.0 °C | 120 - 150 W/(m·K) Show Supplier Material materials with Conductividad térmica of 120 - 150 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.80E+7 - 2.20E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.80E+7 - 2.20E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Heat treatable alloy | |
Processing history | Temper: T651 |