General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.75 g/cm³ Show Supplier Material materials with Densidad of 2.75 g/cm³ |
Rugosidad superficial | 0.4 μm Show Supplier Material materials with Rugosidad superficial of 0.4 μm |
Medidas
Property | Value |
---|---|
Dimensions | Standard stock sizes: 1520mm x 3020mm and 8-80mm in thickness |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell (HBW) | 23.0 °C | 125 - 130 [-] Show Supplier Material materials with Dureza Brinell (HBW) of 125 - 130 [-] | Test method: 2.5/62.5 |
Elongación A50 | 23.0 °C | 8 - 13 % Show Supplier Material materials with Elongación A50 of 8 - 13 % | |
Límite elástico Rp 0,2 | 23.0 °C | 330 - 370 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 330 - 370 MPa | |
Módulo elástico | 23.0 °C | 71 GPa Show Supplier Material materials with Módulo elástico of 71 GPa | |
Resistencia a la tracción | 23.0 °C | 390 - 420 MPa Show Supplier Material materials with Resistencia a la tracción of 390 - 420 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 875 J/(kg·K) Show Supplier Material materials with Calor específico of 875 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.36E-5 1/K |
Conductividad térmica | 23.0 °C | 135 - 150 W/(m·K) Show Supplier Material materials with Conductividad térmica of 135 - 150 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.90E+7 - 2.30E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.90E+7 - 2.30E+7 S/m |
Technological properties
Property | ||
---|---|---|
Other | Non heat treatable | |
Processing history | Temper: T651 |