Our own graphene inks are produced via a patented micro-fluidisation process. Printable conductive inks for flexible electronics can be both cheaper and more flexible than traditional circuit board solutions. We have two different inks suitable for different deposition methods. Both are environmentally friendly, non-toxic, aqueous and can be stored at room temperature (20°C). We also formulate graphene inks for specific customer requirements. Solvent: Water, Solid content: 0.1 wt%, Graphene content: 0.2-0.5 mg/mL, Transparent films can be coated, Transparent substrates: Glass, Paper and Plastics

Los datos sobre este material han sido proporcionados por Versarien.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

General

PropertyValue

Espesor de la capa

0.003

Show Supplier Material materials with Espesor de la capa of 0.003

Tamaño de lámina lateral

80.0 - 500.0 nm

Show Supplier Material materials with Tamaño de lámina lateral of 80.0 - 500.0 nm

Eléctrico

PropertyValueComment

Surface resistivity

30.0 - 4000.0 Ω/sq

Show Supplier Material materials with Surface resistivity of 30.0 - 4000.0 Ω/sq

Minimum for 80nm and Maximum for 2µm thickness

Rheological Properties

PropertyValue

Viscosidad

0.003 Pa·s

Show Supplier Material materials with Viscosidad of 0.003 Pa·s

Technological properties

Property
Application areas

flexible electronics

Processing methods

Ink jet printing, Vacuum Filtration, Meyer Bar Coating - with a drying condition of 100℃ for 10 min