General
Property | Value |
---|---|
Densidad relativa | 8.78 [-] Show Supplier Material materials with Densidad relativa of 8.78 [-] |
Mecánica
Property | Value | Comment |
---|---|---|
Dureza Vickers | 223 [-] Show Supplier Material materials with Dureza Vickers of 223 [-] | H Temper |
245 [-] Show Supplier Material materials with Dureza Vickers of 245 [-] | EH Temper | |
267 [-] Show Supplier Material materials with Dureza Vickers of 267 [-] | SH Temper | |
285 [-] Show Supplier Material materials with Dureza Vickers of 285 [-] | ESH Temper | |
305 [-] Show Supplier Material materials with Dureza Vickers of 305 [-] | XSH Temper | |
Elongación | 2 % Show Supplier Material materials with Elongación of 2 % | XSH Temper |
2.4 % Show Supplier Material materials with Elongación of 2.4 % | ESH Temper | |
9.2 % Show Supplier Material materials with Elongación of 9.2 % | SH Temper | |
15.3 % Show Supplier Material materials with Elongación of 15.3 % | EH Temper | |
25.6 % Show Supplier Material materials with Elongación of 25.6 % | H Temper | |
Límite elástico | 558 MPa Show Supplier Material materials with Límite elástico of 558 MPa | H Temper | for spring material (Kb0.1) |
585 MPa Show Supplier Material materials with Límite elástico of 585 MPa | EH Temper | for spring material (Kb0.1) | |
657 MPa Show Supplier Material materials with Límite elástico of 657 MPa | H Temper, RP02 | |
661 MPa Show Supplier Material materials with Límite elástico of 661 MPa | SH Temper | for spring material (Kb0.1) | |
718 MPa Show Supplier Material materials with Límite elástico of 718 MPa | ESH Temper | for spring material (Kb0.1) | |
783 MPa Show Supplier Material materials with Límite elástico of 783 MPa | EH Temper, RP02 | |
877 MPa Show Supplier Material materials with Límite elástico of 877 MPa | SH Temper, RP02 | |
883 MPa Show Supplier Material materials with Límite elástico of 883 MPa | XSH Temper | for spring material (Kb0.1) | |
988 MPa Show Supplier Material materials with Límite elástico of 988 MPa | ESH Temper, RP02 | |
1044 MPa Show Supplier Material materials with Límite elástico of 1044 MPa | XSH Temper, RP02 | |
Módulo de flexión | 100 GPa Show Supplier Material materials with Módulo de flexión of 100 GPa | |
Módulo elástico | 105 GPa Show Supplier Material materials with Módulo elástico of 105 GPa | |
Plegabilidad 90 ° bidireccional | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 0 [-] | H Temper |
1.5 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 1.5 [-] | EH Temper | |
2 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 2 [-] | SH Temper | |
3.3 [-] Show Supplier Material materials with Plegabilidad 90 ° bidireccional of 3.3 [-] | ESH Temper | |
Plegabilidad 90 ° en peso bruto | 0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | H Temper |
0 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0 [-] | EH Temper | |
0.8 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 0.8 [-] | SH Temper | |
1.6 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 1.6 [-] | ESH Temper | |
2.5 [-] Show Supplier Material materials with Plegabilidad 90 ° en peso bruto of 2.5 [-] | XSH Temper | |
Resistencia a la tracción | 693 MPa Show Supplier Material materials with Resistencia a la tracción of 693 MPa | H Temper |
800 MPa Show Supplier Material materials with Resistencia a la tracción of 800 MPa | EH Temper | |
890 MPa Show Supplier Material materials with Resistencia a la tracción of 890 MPa | SH Temper | |
1000 MPa Show Supplier Material materials with Resistencia a la tracción of 1000 MPa | ESH Temper | |
1058 MPa Show Supplier Material materials with Resistencia a la tracción of 1058 MPa | XSH Temper |
Aplicaciones térmicas
Property | Value |
---|---|
Calor específico | 375 J/(kg·K) Show Supplier Material materials with Calor específico of 375 J/(kg·K) |
Coeficiente de dilatación térmica | 1.84e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.84e-05 1/K |
Conductividad térmica | 50 W/(m·K) Show Supplier Material materials with Conductividad térmica of 50 W/(m·K) |
Temperatura de fusión | 845 - 1000 °C Show Supplier Material materials with Temperatura de fusión of 845 - 1000 °C |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 10 % IACS Show Supplier Material materials with Specific Electrical conductivity of 10 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Estaño | 9 - 11 % Show Supplier Material materials with Estaño of 9 - 11 % | |
Fósforo | 0.04 - 0.2 % Show Supplier Material materials with Fósforo of 0.04 - 0.2 % | |
Hierro | 0.01 % Show Supplier Material materials with Hierro of 0.01 % | max. |
Otro | 99.8 % Show Supplier Material materials with Otro of 99.8 % | min. | Cu+Sn+P |
Plomo | 0.01 % Show Supplier Material materials with Plomo of 0.01 % | max. |
Zinc | 0.01 % Show Supplier Material materials with Zinc of 0.01 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Please contact the supplier if you have any specific requests regarding chemical compostions, mechanical properties, and thickness. | |
Tolerances |