General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 18.8 g/cm³ Show Supplier Material materials with Densidad of 18.8 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 370 - 420 [-] Show Supplier Material materials with Dureza Vickers of 370 - 420 [-] |
Elongación | 23.0 °C | 1 - 2 % Show Supplier Material materials with Elongación of 1 - 2 % |
Límite elástico Rp 0,2 | 23.0 °C | 1050 - 1200 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 1050 - 1200 MPa |
Módulo de cizallamiento | 23.0 °C | 74 GPa Show Supplier Material materials with Módulo de cizallamiento of 74 GPa |
Módulo elástico | 23.0 °C | 180 GPa Show Supplier Material materials with Módulo elástico of 180 GPa |
Resistencia a la tracción | 23.0 °C | 1160 - 1230 MPa Show Supplier Material materials with Resistencia a la tracción of 1160 - 1230 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.02E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.02E-5 1/K | RT-100 °C |
Temperatura de fusión | 1660 - 1700 °C Show Supplier Material materials with Temperatura de fusión of 1660 - 1700 °C |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de temperatura de la resistencia | 23.0 °C | 1.25E-3 - 1.35E-3 1/K Show Supplier Material materials with Coeficiente de temperatura de la resistencia of 1.25E-3 - 1.35E-3 1/K | 0-100 °C |
Resistividad eléctrica | 23.0 °C | 2.98E-7 - 3.04E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.98E-7 - 3.04E-7 Ω·m | |
Specific Electrical conductivity | 5.6 - 5.77 % IACS Show Supplier Material materials with Specific Electrical conductivity of 5.6 - 5.77 % IACS |
Technological properties
Property | ||
---|---|---|
Application areas | Spark plugs, electrodes | |
Corrosion properties | Corrosion resistant | |
Other | Ductile |