General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.15 g/cm³ Show Material materials with Densidad of 2.15 g/cm³ | DIN EN ISO 12086 |
Densidad aparente | 23.0 °C | 0.87 g/cm³ Show Material materials with Densidad aparente of 0.87 g/cm³ | DIN EN ISO 60 |
Tamaño de partícula | 220000 nm Show Material materials with Tamaño de partícula of 220000 nm | ISO 13320, average value |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 56 [-] Show Material materials with Dureza Shore D of 56 [-] | DIN EN ISO 868 |
Elongación | 23.0 °C | 400 % Show Material materials with Elongación of 400 % | DIN EN ISO 527-3, 0.2 mm film |
Módulo elástico | 23.0 °C | 0.6 GPa Show Material materials with Módulo elástico of 0.6 GPa | DIN EN ISO 527 |
Resistencia a la tracción | 23.0 °C | 38 MPa Show Material materials with Resistencia a la tracción of 38 MPa | DIN EN ISO 527-3, 0.2 mm film |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 100.0 °C | 1.2E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | ||
200.0 °C | 1.4E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
260.0 °C | 1.7E-4 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-4 1/K | DIN 53 752, from 30°C to the mentioned temperature | |||
Conductividad térmica | 23.0 °C | 0.22 W/(m·K) Show Material materials with Conductividad térmica of 0.22 W/(m·K) | DIN 52612 | ||
Inflamabilidad | V-0 UL94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.00E+16 Ω·m Show Material materials with Resistividad eléctrica of 1.00E+16 Ω·m | IEC 60093 |
Rigidez dieléctrica | 23.0 °C | 74 kV/mm Show Material materials with Rigidez dieléctrica of 74 kV/mm | DIN EN ISO 12086, 0.2 mm film |
Surface resistivity | 23.0 °C | 1.00E+17 Ω/sq Show Material materials with Surface resistivity of 1.00E+17 Ω/sq | IEC 60093 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 2.9 % Show Material materials with Contracción of 2.9 % | Internal Dyneon method, Cylinder 45 mm diameter |
Technological properties
Property | ||
---|---|---|
Application areas | 3MTM DyneonTM PTFE Granules TF 1620 is a semi-free-flowing compression moulding powder for applications like large compression moulded sheets, isostatically moulded articles, shaped parts, thinner wall articles (like bellows etc.) and for skived films of > 200 μm. |