General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.44 g/cm³ Show Material materials with Densidad of 1.44 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 3 % Show Material materials with Elongación of 3 % | ISO 527 | 5 mm/min |
Hardness, Ball Indentation | 23.0 °C | 100 MPa Show Material materials with Hardness, Ball Indentation of 100 MPa | ISO 2039-1 |
Hardness, Rockwell R | 23.0 °C | 109 [-] Show Material materials with Hardness, Rockwell R of 109 [-] | ISO 2039-2 |
Módulo de flexión | 23.0 °C | 7.75 GPa Show Material materials with Módulo de flexión of 7.75 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 8.5 GPa Show Material materials with Módulo elástico of 8.5 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 160 MPa Show Material materials with Resistencia a la flexión of 160 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 105 MPa Show Material materials with Resistencia a la tracción of 105 MPa | ISO 527 | 5 mm/min |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 16 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 16 kJ/m² | ISO 179/2C |
Resistencia al choque, ensayo Charpy no entallado | -30.0 °C | 22 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 22 kJ/m² | ISO 179/1eU |
23.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 35 kJ/m² | ISO 179/1eU | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 6 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 6 kJ/m² | ISO 180/1A |
23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 10 kJ/m² | ISO 180/1A | |
Resistencia al choque, ensayo Izod no entallado | -30.0 °C | 42 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 42 kJ/m² | ISO 180/1U |
23.0 °C | 44 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 44 kJ/m² | ISO 180/1U | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K | ISO 11359-2 | -23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 1.1E-4 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 1.1E-4 1/K | ISO 11359-2 | 23°C to 80°C | ||
Conductividad térmica | 23.0 °C | 0.19 W/(m·K) Show Material materials with Conductividad térmica of 0.19 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 140 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 140 °C | ISO 75/Ae | 1.8 MPa | |||
Relative temperature index, electrical | 140 °C Show Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||
Relative temperature index, mechanical impact | 130 °C Show Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |||
Relative temperature index, mechanical strength | 140 °C Show Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 150 °C Show Material materials with Temperatura de reblandecimiento Vicat of 150 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating 2nd value | 3mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.7 [-] Show Material materials with Constante dieléctrica of 3.7 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 0.02 [-] Show Material materials with Factor de disipación of 0.02 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 15 kV/mm Show Material materials with Rigidez dieléctrica of 15 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Índice de seguimiento comparativo | 23.0 °C | 300 V Show Material materials with Índice de seguimiento comparativo of 300 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 - 0.6 % Show Material materials with Contracción of 0.3 - 0.6 % | SABIC method |
Contracción transversal | 23.0 °C | 0.4 - 0.8 % Show Material materials with Contracción transversal of 0.4 - 0.8 % | SABIC method |
Velocidad de flujo del volumen derretido | 12 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 12 cm³/10min | ISO 1133 | 250°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Cooking Range,Data Transfer,Electronic Components,Enclosures,EV Infrastructure,Exterior,Forward Lighting,Heavy Vehicles,Individual Equiptment,Medical Facility Infrastructure,Motorcycle,Personal Computing,Small Appliance,Swimming Pool/Spa,Wireless Communications | |
Processing methods | Drying Temperature: 100-110°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 255-270°C, Nozzle Temperature: 250-265°C, Front - Zone 3 Temperature: 250-270°C, Middle - Zone 2 Temperature: 240-265°C, Rear - Zone 1 Temperature: 230-250°C, Hopper Temperature: 40-60°C, Mold Temperature: 60-100°C |