General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.15 % Show Material materials with Absorción de agua of 0.15 % | ISO 62 | 23°C, 50% RH |
Densidad | 23.0 °C | 1.22 g/cm³ Show Material materials with Densidad of 1.22 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Elongación | 23.0 °C | 120 % Show Material materials with Elongación of 120 % | ISO 527 | 50 mm/min | ||
Flexural yield strength | 23.0 °C | 80 MPa Show Material materials with Flexural yield strength of 80 MPa | ISO 178 | 2 mm/min | ||
Límite elástico | 23.0 °C | 50 MPa Show Material materials with Límite elástico of 50 MPa | ISO 527 | 50 mm/min | ||
Módulo de flexión | 23.0 °C | 2 GPa Show Material materials with Módulo de flexión of 2 GPa | ISO 178 | 2 mm/min | ||
Módulo elástico | 23.0 °C | 2.05 GPa Show Material materials with Módulo elástico of 2.05 GPa | ISO 527 | 1 mm/min | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 35 kJ/m² | ISO 179/1eA | ||
23.0 °C | 55 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 55 kJ/m² | ISO 179/1eA | |||
Resistencia al choque, ensayo Izod entallado | -40.0 °C | 20 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 20 kJ/m² | ISO 180/1A | ||
-30.0 °C | 30 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 30 kJ/m² | ISO 180/1A | |||
23.0 °C | 50 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 50 kJ/m² | ISO 180/1A | |||
Resistencia al choque, ensayo Charpy no entallado | No Break @ 23,-30°C | ISO 179/1eU | ||||
Resistencia al choque, ensayo Izod no entallado | No Break @ 23,-30°C| ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9E-5 1/K | ISO 11359-2 | -23°C to 80°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 9.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 9.5E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 82 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Ae | 1.8 MPa | |||
Relative temperature index, electrical | 75 °C Show Material materials with Relative temperature index, electrical of 75 °C | UL 746B | |||
Relative temperature index, mechanical impact | 75 °C Show Material materials with Relative temperature index, mechanical impact of 75 °C | UL 746B | |||
Relative temperature index, mechanical strength | 75 °C Show Material materials with Relative temperature index, mechanical strength of 75 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 125 °C Show Material materials with Temperatura de reblandecimiento Vicat of 125 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating | 1.5mm | UL 94 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Constante dieléctrica | 23.0 °C | 3.3 [-] Show Material materials with Constante dieléctrica of 3.3 [-] | IEC 60250 | at 50/60 Hz |
Factor de disipación | 23.0 °C | 0.02 [-] Show Material materials with Factor de disipación of 0.02 [-] | IEC 60250 | at 1 MHz |
Rigidez dieléctrica | 23.0 °C | 17 kV/mm Show Material materials with Rigidez dieléctrica of 17 kV/mm | IEC 60243-1 | in oil, 3.2 mm |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.7 - 1.1 % Show Material materials with Contracción of 0.7 - 1.1 % | SABIC method |
Contracción transversal | 23.0 °C | 0.8 - 1.1 % Show Material materials with Contracción transversal of 0.8 - 1.1 % | SABIC method |
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | ISO 1133 | 250°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Audio,Auto Aftermarket,Body Protection,Building Accessory,Building Element,Data Management,Data Transfer,Defense Vehicles,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exterior Mirror,Exterior,Food Container,Head Protection,Heavy Vehicles,Hygiene/Personal Care,Individual Equiptment,Industrial Material Handling,Interior,Lab Ware and Clinical Diagnostics,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Gas,Neighborhood Electric Vehicle,Non-LED Lighting,Personal Computing,Power Boat,Power Manangement,Pump,Recreational Vehicle,Respiratory,Security/Detection,Small Appliance,Storage/Table,Surgical Devices,Swimming Pool/Spa,Traffic Management,Travel Suitcase,Water Treatment/Filtration,Wearables,Wireless Communications,Wiring Devices,Wire & cable | |
Processing methods | Drying Temperature: 90-100°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 255-270°C, Nozzle Temperature: 250-265°C, Front - Zone 3 Temperature: 250-270°C, Middle - Zone 2 Temperature: 240-265°C, Rear - Zone 1 Temperature: 230-250°C, Hopper Temperature: 40-60°C, Mold Temperature: 60-80°C |