General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.08 g/cm³ Show Material materials with Densidad of 1.08 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 10 % Show Material materials with Elongación of 10 % | ISO 527 | 50 mm/min |
Elongation at yield | 23.0 °C | 3.4 % Show Material materials with Elongation at yield of 3.4 % | ISO 527 | 50 mm/min |
Flexural yield strength | 23.0 °C | 69 MPa Show Material materials with Flexural yield strength of 69 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 91 MPa Show Material materials with Hardness, Ball Indentation of 91 MPa | ISO 2039-1 |
Límite elástico | 23.0 °C | 45 MPa Show Material materials with Límite elástico of 45 MPa | ISO 527 | 50 mm/min |
Módulo de flexión | 23.0 °C | 2.25 GPa Show Material materials with Módulo de flexión of 2.25 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 2.2 GPa Show Material materials with Módulo elástico of 2.2 GPa | ISO 527 | 1 mm/min |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 14 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 14 kJ/m² | ISO 179/1eA |
23.0 °C | 34 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 34 kJ/m² | ISO 179/1eA | |
Resistencia al choque, ensayo Izod entallado | -30.0 °C | 15 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 15 kJ/m² | ISO 180/1A |
23.0 °C | 35 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 35 kJ/m² | ISO 180/1A | |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 9.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Coeficiente de dilatación térmica transversal | 23.0 °C | 9.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica transversal of 9.8E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Conductividad térmica | 23.0 °C | 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.2 W/(m·K) | ISO 8302 | ||
Heat deflection temperature, 1.80 MPa | 87 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 87 °C | ISO 75/Ae | 1.8 MPa | |||
Relative temperature index, electrical | 60 °C Show Material materials with Relative temperature index, electrical of 60 °C | UL 746B | |||
Relative temperature index, mechanical impact | 60 °C Show Material materials with Relative temperature index, mechanical impact of 60 °C | UL 746B | |||
Relative temperature index, mechanical strength | 60 °C Show Material materials with Relative temperature index, mechanical strength of 60 °C | UL 746B | |||
Temperatura de reblandecimiento Vicat | 107 °C Show Material materials with Temperatura de reblandecimiento Vicat of 107 °C | ISO 306 | Rate B/120 | |||
Inflamabilidad | UL Recognized, 94HB Flame Class Rating 2nd value | 3mm | UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 - 0.7 % Show Material materials with Contracción of 0.5 - 0.7 % | SABIC method |
Velocidad de flujo del volumen derretido | 8 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 8 cm³/10min | ISO 1133 | 260°C/5.0 kg |
Technological properties
Property | ||
---|---|---|
Application areas | ATM/Ticket Machine,Auto Aftermarket,Cluster,Console,Displays,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,Exterior Trim,Front Grille,HVAC Underhood,Interior,Long Distance Coach,Meter Gas,Motorcycle,Rail Cabin Interiors,Rear/Signal Lighting,Recreational Vehicle,Seat,Small Appliance,Travel Suitcase,Trim | |
Processing methods | Drying Temperature: 90-100°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.1%, Melt Temperature: 250-280°C, Nozzle Temperature: 245-275°C, Front - Zone 3 Temperature: 250-280°C, Middle - Zone 2 Temperature: 250-280°C, Rear - Zone 1 Temperature: 230-260°C, Hopper Temperature: 60-80°C, Mold Temperature: 40-80°C |