General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.95 g/cm³ Show Material materials with Densidad of 0.95 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 62 [-] Show Material materials with Dureza Shore D of 62 [-] | ASTM D2240 |
Elongation at yield | 23.0 °C | 8 % Show Material materials with Elongation at yield of 8 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 22 MPa Show Material materials with Límite elástico of 22 MPa | ASTM D638 |
Módulo de flexión | 23.0 °C | 0.6 GPa Show Material materials with Módulo de flexión of 0.6 GPa | ISO 178/1A |
Módulo elástico | 23.0 °C | 0.85 GPa Show Material materials with Módulo elástico of 0.85 GPa | ASTM D638 |
Resistencia a la flexión | 23.0 °C | 19 MPa Show Material materials with Resistencia a la flexión of 19 MPa | ISO 178 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 23 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 23 kJ/m² | ISO 179 |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 74 °C Show Material materials with Temperatura de reblandecimiento Vicat of 74 °C | ISO 306 | 50N (VST/B) |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe |