General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.96 g/cm³ Show Material materials with Densidad of 0.96 g/cm³ | ASTM D1505 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore D | 23.0 °C | 59 [-] Show Material materials with Dureza Shore D of 59 [-] | ISO 868 |
Elongation at yield | 23.0 °C | 8 % Show Material materials with Elongation at yield of 8 % | ISO 527-1/-2 |
Límite elástico | 23.0 °C | 22 MPa Show Material materials with Límite elástico of 22 MPa | ISO 527-1/-2 |
Módulo elástico | 23.0 °C | 0.85 GPa Show Material materials with Módulo elástico of 0.85 GPa | ASTM D638 |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 8 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO 179 |
23.0 °C | 24 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 24 kJ/m² | ISO 179 | |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de reblandecimiento Vicat | 70 °C Show Material materials with Temperatura de reblandecimiento Vicat of 70 °C | ISO 306 | 50 N (VST/B) |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for pipe extrusion while it is particularly suitable for drinking water and waste water piping. Also used for chemical apparatus and containers. |