Common features of Crastin® thermoplastic polyester resin include mechanical and physical properties such as stiffness and toughness, heat resistance, friction and wear resistance, excellent surface finishes and good colourability. Crastin® thermoplastic polyester resin has excellent electrical insulation characteristics and high arc-resistant grades are available. Many flame retardant grades have UL recognition (class V-0). Crastin® thermoplastic polyester resin typically has high chemical and heat ageing resistance. The good melt stability of Crastin® thermoplastic polyester resin normally enables the recycling of properly handled production waste.If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.Crastin® thermoplastic polyester resin typically is used in demanding applications in the electronics, electrical, automotive, mechanical engineering, chemical, domestic appliances and sporting goods industry.Crastin® LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warpage characteristics.

Los datos sobre este material han sido proporcionados por Matmatch.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValueComment

Absorción de agua

23.0 °C

0.72 %

Show Material materials with Absorción de agua of 0.72 %

Sim. to ISO 62 | 80mil

Densidad

23.0 °C

1.44 g/cm³

Show Material materials with Densidad of 1.44 g/cm³

ISO 1183

Mecánica

PropertyTemperatureValueComment

Coeficiente de Poisson

23.0 °C

0.34 [-]

Show Material materials with Coeficiente de Poisson of 0.34 [-]

Elongación

23.0 °C

2.5 %

Show Material materials with Elongación of 2.5 %

ISO 527-1/-2

Módulo de flexión

23.0 °C

8.5 GPa

Show Material materials with Módulo de flexión of 8.5 GPa

ISO 178

Módulo elástico

23.0 °C

9.5 GPa

Show Material materials with Módulo elástico of 9.5 GPa

ISO 527-1/-2

Resistencia a la flexión

23.0 °C

190 MPa

Show Material materials with Resistencia a la flexión of 190 MPa

ISO 178

Resistencia a la tracción

23.0 °C

130 MPa

Show Material materials with Resistencia a la tracción of 130 MPa

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-6.0 °C

9 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m²

ISO 179/1eA

23.0 °C

10 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m²

ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

-6.0 °C

65 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m²

ISO 179/1eU

23.0 °C

60 kJ/m²

Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 60 kJ/m²

ISO 179/1eU

Unlock all property charts

Resistencia al choque, ensayo Izod entallado

-30.0 °C

50 kJ/m²

Show Material materials with Resistencia al choque, ensayo Izod entallado of 50 kJ/m²

ISO 180/1U

23.0 °C

50 kJ/m²

Show Material materials with Resistencia al choque, ensayo Izod entallado of 50 kJ/m²

ISO 180/1U

Unlock all property charts

Resistencia al choque, ensayo Izod no entallado

-30.0 °C

8 kJ/m²

Show Material materials with Resistencia al choque, ensayo Izod no entallado of 8 kJ/m²

ISO 180/1A

23.0 °C

8 kJ/m²

Show Material materials with Resistencia al choque, ensayo Izod no entallado of 8 kJ/m²

ISO 180/1A

Unlock all property charts

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

23.0 °C

1900 J/(kg·K)

Show Material materials with Calor específico of 1900 J/(kg·K)

of melt

Coeficiente de dilatación térmica

23.0 °C

2.5E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 1/K

ISO 11359-1/-2

Coeficiente de dilatación térmica transversal

23.0 °C

1E-4 1/K

Show Material materials with Coeficiente de dilatación térmica transversal of 1E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

215 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 215 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

170 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 170 °C

ISO 75-1/-2

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B | 240mil

Relative temperature index, mechanical impact

130 °C

Show Material materials with Relative temperature index, mechanical impact of 130 °C

UL 746B | 240mil

Relative temperature index, mechanical strength

130 °C

Show Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B | 240mil

Temperatura de fusión

225 °C

Show Material materials with Temperatura de fusión of 225 °C

ISO 11357-1/-3 | 18°F/min

Temperatura de reblandecimiento Vicat

150 °C

Show Material materials with Temperatura de reblandecimiento Vicat of 150 °C

ISO 306 | 90°F/h, 11 lbf

Temperatura de transición del vidrio

120 °C

Show Material materials with Temperatura de transición del vidrio of 120 °C

ISO 11357-1/-2 | 18°F/min

Inflamabilidad

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 3 mm, UL recognition: yes -, Oxygen index: 19 %, Glow Wire Flammability Index, 120mil: 675 °C, Glow Wire Ignition Temperature, 120mil: 675 °C, FMVSS Class: B -, Burning rate, Thickness 1 mm: 42 mm/min

Eléctrico

PropertyTemperatureValueComment

Constante dieléctrica, 1 MHz

23.0 °C

3.6 [-]

Show Material materials with Constante dieléctrica, 1 MHz of 3.6 [-]

IEC 62631-2-1

Constante dieléctrica, 100 Hz

23.0 °C

3.9 [-]

Show Material materials with Constante dieléctrica, 100 Hz of 3.9 [-]

IEC 62631-2-1

Dissipation factor, 100Hz

23.0 °C

2.4E-3 [-]

Show Material materials with Dissipation factor, 100Hz of 2.4E-3 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Material materials with Dissipation factor, 1MHz of 0.02 [-]

IEC 62631-2-1

Rigidez dieléctrica

23.0 °C

21 kV/mm

Show Material materials with Rigidez dieléctrica of 21 kV/mm

IEC 60243-1 | Short Time, 2mm

Surface resistivity

23.0 °C

1.00E+14 Ω/sq

Show Material materials with Surface resistivity of 1.00E+14 Ω/sq

IEC 62631-3-2

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Material materials with Volume resistivity of 1.00E+15 Ω·cm

min. | IEC 62631-3-1

Índice de seguimiento comparativo

23.0 °C

425 V

Show Material materials with Índice de seguimiento comparativo of 425 V

IEC 60112

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.2 %

Show Material materials with Contracción of 0.2 %

ISO 294-4, 2577

Contracción transversal

23.0 °C

0.7 %

Show Material materials with Contracción transversal of 0.7 %

ISO 294-4, 2577

Velocidad de flujo de la masa derretida

10 g/10min

Show Material materials with Velocidad de flujo de la masa derretida of 10 g/10min

ISO 1133 | 250°C/5kg

Technological properties

Property
Fillers

30% Glass Fiber

Processing methods

Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 3s/mm, Back pressure: As low as possible, Ejection temperature: 170°C