General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.35 % Show Material materials with Absorción de agua of 0.35 % | Sim. to ISO 62 | 80mil |
Densidad | 23.0 °C | 1.53 g/cm³ Show Material materials with Densidad of 1.53 g/cm³ | ISO 1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | |
Elongación | 23.0 °C | 2.7 % Show Material materials with Elongación of 2.7 % | ISO 527-1/-2 |
Hardness, Ball Indentation | 23.0 °C | 205 MPa Show Material materials with Hardness, Ball Indentation of 205 MPa | ISO 2039-1 |
Módulo de flexión | 23.0 °C | 9 GPa Show Material materials with Módulo de flexión of 9 GPa | ISO 178 |
Módulo elástico | 23.0 °C | 10 GPa Show Material materials with Módulo elástico of 10 GPa | ISO 527-1/-2 |
Resistencia a la flexión | 23.0 °C | 200 MPa Show Material materials with Resistencia a la flexión of 200 MPa | ISO 178 |
Resistencia a la tracción | 23.0 °C | 140 MPa Show Material materials with Resistencia a la tracción of 140 MPa | ISO 527-1/-2 |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 10 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 65 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | ISO 179/1eU |
Resistencia al choque, ensayo Izod entallado | -40.0 °C | 55 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 55 kJ/m² | ISO 180/1U |
-30.0 °C | 55 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 55 kJ/m² | ISO 180/1U | |
23.0 °C | 60 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod entallado of 60 kJ/m² | ISO 180/1U | |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 9 kJ/m² Show Material materials with Resistencia al choque, ensayo Izod no entallado of 9 kJ/m² | ISO 180/1A |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Calor específico | 23.0 °C | 1730 J/(kg·K) Show Material materials with Calor específico of 1730 J/(kg·K) | of melt | ||
Heat deflection temperature, 1.80 MPa | 205 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75-1/-2 | |||
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | 240mil | |||
Relative temperature index, mechanical impact | 130 °C Show Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | 240mil | |||
Relative temperature index, mechanical strength | 130 °C Show Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | 240mil | |||
Temperatura de fusión | 225 °C Show Material materials with Temperatura de fusión of 225 °C | ISO 11357-1/-3 | 18°F/min | |||
Inflamabilidad | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, UL recognition: yes -, Oxygen index: 20 %, Glow Wire Flammability Index, 30mil: 725 °C, Glow Wire Flammability Index, 60mil: 725 °C, Glow Wire Flammability Index, 120mil: 750 °C, Glow Wire Ignition Temperature, 30mil: 750 °C, Glow Wire Ignition Temperature, 60mil: 750 °C, Glow Wire Ignition Temperature, 120mil: 775 °C, FMVSS Class: B -, Burning rate, Thickness 1 mm: 54 mm/min |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Índice de seguimiento comparativo | 23.0 °C | 225 V Show Material materials with Índice de seguimiento comparativo of 225 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.3 % Show Material materials with Contracción of 0.3 % | ISO 294-4, 2577 |
Contracción transversal | 23.0 °C | 1.1 % Show Material materials with Contracción transversal of 1.1 % | ISO 294-4, 2577 |
Velocidad de flujo de la masa derretida | 10 g/10min Show Material materials with Velocidad de flujo de la masa derretida of 10 g/10min | ISO 1133 | 250°C/2.16kg | |
Velocidad de flujo del volumen derretido | 7 cm³/10min Show Material materials with Velocidad de flujo del volumen derretido of 7 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 3s/mm, Back pressure: As low as possible, Ejection temperature: 170°C |