General
Property | Value |
---|---|
Densidad | 1.17 - 1.24 g/cm³ Show Material materials with Densidad of 1.17 - 1.24 g/cm³ |
Mecánica
Property | Value | Comment | |
---|---|---|---|
Elongación | 80.0 - 150.0 % Show Material materials with Elongación of 80.0 - 150.0 % | ||
Módulo elástico | 1.8 - 2.5 GPa Show Material materials with Módulo elástico of 1.8 - 2.5 GPa | ||
Resistencia a la tracción | 40.0 - 65.0 MPa Show Material materials with Resistencia a la tracción of 40.0 - 65.0 MPa | at 4-6% strain | |
Resistencia al choque, ensayo Charpy entallado | 40.0 - 70.0 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 40.0 - 70.0 kJ/m² | ||
Resistencia al choque, ensayo Charpy no entallado | no break |
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 8e-05 - 0.00011 1/K Show Material materials with Coeficiente de dilatación térmica of 8e-05 - 0.00011 1/K |
Conductividad térmica | 0.18 - 0.2 W/(m·K) Show Material materials with Conductividad térmica of 0.18 - 0.2 W/(m·K) |
Temperatura de fusión | 220.0 - 225.0 °C Show Material materials with Temperatura de fusión of 220.0 - 225.0 °C |
Inflamabilidad | UL 94 HB |
Eléctrico
Property | Value |
---|---|
Constante dieléctrica | 3 [-] Show Material materials with Constante dieléctrica of 3 [-] |
3.5 [-] Show Material materials with Constante dieléctrica of 3.5 [-] | |
Resistividad eléctrica | 10000000000000.0 - 1000000000000000.0 Ω·m Show Material materials with Resistividad eléctrica of 10000000000000.0 - 1000000000000000.0 Ω·m |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Body panels, doorhandles, medical device enclosures, outdoor sport equipment | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding |