General
Property | Value |
---|---|
Densidad | 1.33 - 1.37 g/cm³ Show Material materials with Densidad of 1.33 - 1.37 g/cm³ |
Mecánica
Property | Value | Comment |
---|---|---|
Elongación | 5.0 - 8.0 % Show Material materials with Elongación of 5.0 - 8.0 % | |
Módulo elástico | 5.5 - 7.5 GPa Show Material materials with Módulo elástico of 5.5 - 7.5 GPa | |
Resistencia a la tracción | 90.0 - 125.0 MPa Show Material materials with Resistencia a la tracción of 90.0 - 125.0 MPa | at 5-8% strain |
Resistencia al choque, ensayo Charpy entallado | 10.0 - 25.0 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy entallado of 10.0 - 25.0 kJ/m² | |
Resistencia al choque, ensayo Charpy no entallado | 80 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 80 kJ/m² | |
100 kJ/m² Show Material materials with Resistencia al choque, ensayo Charpy no entallado of 100 kJ/m² |
Aplicaciones térmicas
Property | Value |
---|---|
Coeficiente de dilatación térmica | 2e-05 - 0.00011 1/K Show Material materials with Coeficiente de dilatación térmica of 2e-05 - 0.00011 1/K |
Temperatura de fusión | 240.0 - 260.0 °C Show Material materials with Temperatura de fusión of 240.0 - 260.0 °C |
Inflamabilidad | UL 94 HB |
Eléctrico
Property | Value |
---|---|
Constante dieléctrica | 4 [-] Show Material materials with Constante dieléctrica of 4 [-] |
9 [-] Show Material materials with Constante dieléctrica of 9 [-] | |
Resistividad eléctrica | 1000000000.0 - 10000000000000.0 Ω·m Show Material materials with Resistividad eléctrica of 1000000000.0 - 10000000000000.0 Ω·m |
Óptico
Property | Value |
---|---|
Transparencia | no |
Technological properties
Property | ||
---|---|---|
Application areas | Carbon brush holders, fuel tank caps, bumper support, oil filler pipes, radiatorcaps, gear wheels | |
Fillers | 30% Glass Fiber | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, extrusion, blow molding |