General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Elongación | 13.4 % Show Material materials with Elongación of 13.4 % | Predicted Value, A200 | ||||
15.3 % Show Material materials with Elongación of 15.3 % | Predicted Value, A80 | |||||
17.6 % Show Material materials with Elongación of 17.6 % | Predicted Value, Transverse | |||||
19.0 % Show Material materials with Elongación of 19.0 % | Predicted Value, A80 Transverse | |||||
20.4 % Show Material materials with Elongación of 20.4 % | Predicted Value, A5 | |||||
22.2 % Show Material materials with Elongación of 22.2 % | Predicted Value, A50 | |||||
20 °C | 17 % Show Material materials with Elongación of 17 % | thermomechanically rolled | EN 10028-5 | Flat | ||
Estricción | 39.6 % Show Material materials with Estricción of 39.6 % | Predicted Value | ||||
44.2 % Show Material materials with Estricción of 44.2 % | Predicted Value, Transverse | |||||
Límite elástico | 261.9 MPa Show Material materials with Límite elástico of 261.9 MPa | Predicted Value, RP1 | ||||
318.9 MPa Show Material materials with Límite elástico of 318.9 MPa | Predicted Value, RP1 Transverse | |||||
430.3 MPa Show Material materials with Límite elástico of 430.3 MPa | Predicted Value, RP02 | |||||
438.9 MPa Show Material materials with Límite elástico of 438.9 MPa | Predicted Value, Transverse | |||||
462.2 MPa Show Material materials with Límite elástico of 462.2 MPa | Predicted Value, RP02 Transverse | |||||
524.6 MPa Show Material materials with Límite elástico of 524.6 MPa | Predicted Value, RP05 | |||||
525.5 MPa Show Material materials with Límite elástico of 525.5 MPa | Predicted Value, RP002 | |||||
20 °C | 430 MPa Show Material materials with Límite elástico of 430 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
20 °C | 440 MPa Show Material materials with Límite elástico of 440 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
20 °C | 460 MPa Show Material materials with Límite elástico of 460 MPa | thermomechanically rolled | EN 10028-5 | Flat | ||
Módulo de cizallamiento | 80.0 GPa Show Material materials with Módulo de cizallamiento of 80.0 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 530 - 720 MPa Show Material materials with Resistencia a la tracción of 530 - 720 MPa | thermomechanically rolled | EN 10028-5 | Flat | |
Resistencia al cizallamiento | 558.2 MPa Show Material materials with Resistencia al cizallamiento of 558.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 453.8 J/(kg·K) Show Material materials with Calor específico of 453.8 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.72 1/K Show Material materials with Coeficiente de dilatación térmica of 11.72 1/K | Predicted Value |
Conductividad térmica | 37.79 W/(m·K) Show Material materials with Conductividad térmica of 37.79 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % | thermomechanically rolled | EN 10028-5 | Flat |
0.02 % Show Material materials with Azufre of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat | |
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % | thermomechanically rolled | EN 10028-5 | Flat |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | thermomechanically rolled | EN 10028-5 | Flat |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % | thermomechanically rolled | EN 10028-5 | Flat |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % | thermomechanically rolled | EN 10028-5 | Flat |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % | thermomechanically rolled | EN 10028-5 | Flat |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % | thermomechanically rolled | EN 10028-5 | Flat |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % | thermomechanically rolled | EN 10028-5 | Flat |
Silicona | 0.6 % Show Material materials with Silicona of 0.6 % | thermomechanically rolled | EN 10028-5 | Flat |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | thermomechanically rolled | EN 10028-5 | Flat |
Vanadio | 0.1 % Show Material materials with Vanadio of 0.1 % | thermomechanically rolled | EN 10028-5 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |