General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
20.0 °C | 2.8 g/cm³ Show Material materials with Densidad of 2.8 g/cm³ | T4 | EN 573-3 | Profile, Rod, Flat, Tube, Wire, Sheet |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Bending Fatigue Strength | 130.0 MPa Show Material materials with Bending Fatigue Strength of 130.0 MPa | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Dureza Brinell | 101.0 [-] Show Material materials with Dureza Brinell of 101.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
108.0 [-] Show Material materials with Dureza Brinell of 108.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
111.0 [-] Show Material materials with Dureza Brinell of 111.0 [-] | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 101.0 - 108.0 [-] Show Material materials with Dureza Brinell of 101.0 - 108.0 [-] | T4 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 101.0 - 105.0 [-] Show Material materials with Dureza Brinell of 101.0 - 105.0 [-] | T4 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 101.0 [-] Show Material materials with Dureza Brinell of 101.0 [-] | T4 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 101.0 - 110.0 [-] Show Material materials with Dureza Brinell of 101.0 - 110.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 101.0 - 111.0 [-] Show Material materials with Dureza Brinell of 101.0 - 111.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 105.0 [-] Show Material materials with Dureza Brinell of 105.0 [-] | T4 | EN 573-3 | Profile, Rod, Tube, Sheet, Flat | ||
20.0 °C | 105.0 - 108.0 [-] Show Material materials with Dureza Brinell of 105.0 - 108.0 [-] | T4 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 105.0 - 110.0 [-] Show Material materials with Dureza Brinell of 105.0 - 110.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 105.0 - 111.0 [-] Show Material materials with Dureza Brinell of 105.0 - 111.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 108.0 [-] Show Material materials with Dureza Brinell of 108.0 [-] | T4 | EN 573-3 | Sheet, Flat | ||
20.0 °C | 108.0 - 110.0 [-] Show Material materials with Dureza Brinell of 108.0 - 110.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 108.0 - 111.0 [-] Show Material materials with Dureza Brinell of 108.0 - 111.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 110.0 [-] Show Material materials with Dureza Brinell of 110.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 110.0 - 111.0 [-] Show Material materials with Dureza Brinell of 110.0 - 111.0 [-] | T4 | EN 573-3 | Flat | ||
20.0 °C | 111.0 [-] Show Material materials with Dureza Brinell of 111.0 [-] | T4 | EN 573-3 | Flat | ||
Elongación | 2.0 % Show Material materials with Elongación of 2.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | |
4.0 % Show Material materials with Elongación of 4.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
6.0 % Show Material materials with Elongación of 6.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
7.0 % Show Material materials with Elongación of 7.0 % | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
8.0 % Show Material materials with Elongación of 8.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
8.0 % Show Material materials with Elongación of 8.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
9.0 % Show Material materials with Elongación of 9.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
10.0 % Show Material materials with Elongación of 10.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
10.0 % Show Material materials with Elongación of 10.0 % | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
12.0 % Show Material materials with Elongación of 12.0 % | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | A100 | ||
13.0 % Show Material materials with Elongación of 13.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
14.0 % Show Material materials with Elongación of 14.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
15.0 % Show Material materials with Elongación of 15.0 % | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | A50 | ||
18.0 % Show Material materials with Elongación of 18.0 % | T4 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | T4 | EN 573-3 | Sheet | ||
20.0 °C | 2.0 % Show Material materials with Elongación of 2.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | T4 | EN 573-3 | Sheet | ||
20.0 °C | 4.0 % Show Material materials with Elongación of 4.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T4 | EN 573-3 | Sheet | ||
20.0 °C | 6.0 % Show Material materials with Elongación of 6.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T4 | EN 573-3 | Sheet, Rod | ||
20.0 °C | 7.0 % Show Material materials with Elongación of 7.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T4 | EN 573-3 | Rod | ||
20.0 °C | 8.0 % Show Material materials with Elongación of 8.0 % | T4 | EN 573-3 | Profile, Tube | A50 | |
20.0 °C | 9.0 % Show Material materials with Elongación of 9.0 % | T4 | EN 573-3 | Rod | ||
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T4 | EN 573-3 | Profile, Rod, Tube | ||
20.0 °C | 10.0 % Show Material materials with Elongación of 10.0 % | T4 | EN 573-3 | Rod, Tube | A50 | |
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | T4 | EN 573-3 | Flat, Sheet, Rod, Tube | ||
20.0 °C | 12.0 % Show Material materials with Elongación of 12.0 % | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 13.0 % Show Material materials with Elongación of 13.0 % | T4 | EN 573-3 | Flat | A50 | |
20.0 °C | 13.0 % Show Material materials with Elongación of 13.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | T4 | EN 573-3 | Flat | A50 | |
20.0 °C | 14.0 % Show Material materials with Elongación of 14.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 15.0 % Show Material materials with Elongación of 15.0 % | T4 | EN 573-3 | Flat | A50 | |
20.0 °C | 15.0 % Show Material materials with Elongación of 15.0 % | T4 | EN 573-3 | Flat | A50 Transverse | |
20.0 °C | 18.0 % Show Material materials with Elongación of 18.0 % | T4 | EN 573-3 | Wire | A100 | |
Módulo de cizallamiento | 27.2 GPa Show Material materials with Módulo de cizallamiento of 27.2 GPa | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
20.0 °C | 26.0 - 28.5 GPa Show Material materials with Módulo de cizallamiento of 26.0 - 28.5 GPa | T4 | EN 573-3 | Profile, Rod, Flat, Tube, Wire, Sheet | ||
Módulo elástico | 72.5 GPa Show Material materials with Módulo elástico of 72.5 GPa | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | ||
20.0 °C | 65.0 - 73.5 GPa Show Material materials with Módulo elástico of 65.0 - 73.5 GPa | T4 | EN 573-3 | Profile, Rod, Flat, Tube, Wire, Sheet | ||
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Resistencia a la tracción | 300.0 MPa Show Material materials with Resistencia a la tracción of 300.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
350.0 MPa Show Material materials with Resistencia a la tracción of 350.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
360.0 MPa Show Material materials with Resistencia a la tracción of 360.0 MPa | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
370.0 MPa Show Material materials with Resistencia a la tracción of 370.0 MPa | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | T4 | EN 573-3, EN 1301, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
385.0 MPa Show Material materials with Resistencia a la tracción of 385.0 MPa | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
390.0 MPa Show Material materials with Resistencia a la tracción of 390.0 MPa | T4 | EN 573-3, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T4 | EN 573-3, EN 755 | Strip, Sheet, Plate, Tube, Bar | |||
20.0 °C | 300.0 MPa Show Material materials with Resistencia a la tracción of 300.0 MPa | T4 | EN 573-3 | Sheet | ||
20.0 °C | 300.0 MPa Show Material materials with Resistencia a la tracción of 300.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | T4 | EN 573-3 | Sheet | ||
20.0 °C | 330.0 MPa Show Material materials with Resistencia a la tracción of 330.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 350.0 MPa Show Material materials with Resistencia a la tracción of 350.0 MPa | T4 | EN 573-3 | Sheet | ||
20.0 °C | 350.0 MPa Show Material materials with Resistencia a la tracción of 350.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 360.0 MPa Show Material materials with Resistencia a la tracción of 360.0 MPa | T4 | EN 573-3 | Sheet, Rod | ||
20.0 °C | 360.0 MPa Show Material materials with Resistencia a la tracción of 360.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 370.0 MPa Show Material materials with Resistencia a la tracción of 370.0 MPa | T4 | EN 573-3 | Sheet, Rod | ||
20.0 °C | 370.0 MPa Show Material materials with Resistencia a la tracción of 370.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 380.0 MPa Show Material materials with Resistencia a la tracción of 380.0 MPa | T4 | EN 573-3 | Profile, Wire, Rod, Tube | ||
20.0 °C | 385.0 MPa Show Material materials with Resistencia a la tracción of 385.0 MPa | T4 | EN 573-3 | Sheet | ||
20.0 °C | 385.0 MPa Show Material materials with Resistencia a la tracción of 385.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 390.0 MPa Show Material materials with Resistencia a la tracción of 390.0 MPa | T4 | EN 573-3 | Flat, Rod | ||
20.0 °C | 390.0 MPa Show Material materials with Resistencia a la tracción of 390.0 MPa | T4 | EN 573-3 | Flat | Transverse | |
20.0 °C | 400.0 MPa Show Material materials with Resistencia a la tracción of 400.0 MPa | T4 | EN 573-3 | Rod, Tube | ||
20.0 °C | 436.0 MPa Show Material materials with Resistencia a la tracción of 436.0 MPa | T4 | EN 573-3 | |||
100.0 °C | 394.0 MPa Show Material materials with Resistencia a la tracción of 394.0 MPa | T4 | EN 573-3 | |||
150.0 °C | 281.0 MPa Show Material materials with Resistencia a la tracción of 281.0 MPa | T4 | EN 573-3 | |||
200.0 °C | 155.0 MPa Show Material materials with Resistencia a la tracción of 155.0 MPa | T4 | EN 573-3 | |||
250.0 °C | 84.0 MPa Show Material materials with Resistencia a la tracción of 84.0 MPa | T4 | EN 573-3 | |||
300.0 °C | 46.0 MPa Show Material materials with Resistencia a la tracción of 46.0 MPa | T4 | EN 573-3 | |||
370.0 °C | 32.0 MPa Show Material materials with Resistencia a la tracción of 32.0 MPa | T4 | EN 573-3 | |||
Ángulo de flexión a 180° | 3.0 °/t Show Material materials with Ángulo de flexión a 180° of 3.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
5.0 °/t Show Material materials with Ángulo de flexión a 180° of 5.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
Ángulo de flexión a 90° | 3.0 °/t Show Material materials with Ángulo de flexión a 90° of 3.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | ||
5.0 °/t Show Material materials with Ángulo de flexión a 90° of 5.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar | |||
8.0 °/t Show Material materials with Ángulo de flexión a 90° of 8.0 °/t | T4 | EN 573-3, EN 485 | Strip, Sheet, Plate, Tube, Bar |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Calor específico | 20.0 °C | 921.0 J/(kg·K) Show Material materials with Calor específico of 921.0 J/(kg·K) | T4 | EN 573-3 | Profile, Rod, Flat, Tube, Wire, Sheet |
Coeficiente de dilatación térmica | 20 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar |
100 °C | 2.3e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 1/K | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
Conductividad térmica | 20.0 °C | 130.0 - 200.0 W/(m·K) Show Material materials with Conductividad térmica of 130.0 - 200.0 W/(m·K) | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Profile, Rod, Flat, Tube, Wire, Sheet, Strip, Plate, Bar |
Temperatura de fusión | 512.0 - 650.0 °C Show Material materials with Temperatura de fusión of 512.0 - 650.0 °C | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Conductividad eléctrica | 20.0 °C | 18000000.0 - 28000000.0 S/m Show Material materials with Conductividad eléctrica of 18000000.0 - 28000000.0 S/m | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Profile, Rod, Flat, Tube, Wire, Sheet, Strip, Plate, Bar |
Resistividad eléctrica | 3.57e-08 - 5.56e-08 Ω·m Show Material materials with Resistividad eléctrica of 3.57e-08 - 5.56e-08 Ω·m | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 3.5 - 4.5 % Show Material materials with Cobre of 3.5 - 4.5 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Sheet, Flat, Profile, Rod, Tube, Wire, Strip, Plate, Bar |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Sheet, Flat, Profile, Rod, Tube, Wire, Strip, Plate, Bar |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % | T4 | EN 573-3 | Sheet, Flat, Profile, Rod, Tube, Wire |
0.70 % Show Material materials with Hierro of 0.70 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Strip, Sheet, Plate, Tube, Bar | |
Magnesio | 0.4 - 1.0 % Show Material materials with Magnesio of 0.4 - 1.0 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Sheet, Flat, Profile, Rod, Tube, Wire, Strip, Plate, Bar |
Manganeso | 0.4 - 1.0 % Show Material materials with Manganeso of 0.4 - 1.0 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Sheet, Flat, Profile, Rod, Tube, Wire, Strip, Plate, Bar |
Silicona | 0.2 - 0.8 % Show Material materials with Silicona of 0.2 - 0.8 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Sheet, Flat, Profile, Rod, Tube, Wire, Strip, Plate, Bar |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % | T4 | EN 573-3, EN 1301, EN 485, EN 755 | Sheet, Flat, Profile, Rod, Tube, Wire, Strip, Plate, Bar |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not suitable, Protective: good | |
Brazing | hard brazing (with flux/ without flux): not suitable / not suitable, friction soldering: acceptable, soft brazing with flux: not suitable | |
Corrosion properties | Seawater: poor, weathering: sufficient | |
Workability | Bending / Spinning (cold): good / acceptable, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) acceptable (O) / acceptable (O) |