General
Property | Value | Comment |
---|---|---|
Densidad | 2.6 - 2.7 g/cm³ Show Material materials with Densidad of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium |
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Conductividad térmica | 60.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Temperatura de fusión | 450.0 - 640.0 °C Show Material materials with Temperatura de fusión of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % | EN 1676 |
0.08 % Show Material materials with Cobre of 0.08 % | EN 1676 | |
Estaño | 0.1 % Show Material materials with Estaño of 0.1 % | EN 1676 |
Hierro | 0.4 % Show Material materials with Hierro of 0.4 % | EN 1676 |
0.45 - 0.9 % Show Material materials with Hierro of 0.45 - 0.9 % | EN 1676 | |
Magnesio | 2.7 - 3.5 % Show Material materials with Magnesio of 2.7 - 3.5 % | EN 1676 |
8.5 - 10.5 % Show Material materials with Magnesio of 8.5 - 10.5 % | EN 1676 | |
Manganeso | 0.45 % Show Material materials with Manganeso of 0.45 % | EN 1676 |
0.55 % Show Material materials with Manganeso of 0.55 % | EN 1676 | |
Níquel | 0.1 % Show Material materials with Níquel of 0.1 % | EN 1676 |
Plomo | 0.1 % Show Material materials with Plomo of 0.1 % | EN 1676 |
Silicona | 0.45 % Show Material materials with Silicona of 0.45 % | EN 1676 |
2.5 % Show Material materials with Silicona of 2.5 % | EN 1676 | |
Titanio | 0.15 % Show Material materials with Titanio of 0.15 % | EN 1676 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | EN 1676 |
0.25 % Show Material materials with Zinc of 0.25 % | EN 1676 |