General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | ||||
Dureza Brinell | 245 [-] Show Material materials with Dureza Brinell of 245 [-] | Predicted Value, Transverse | ||||
Elongación | 17.2 % Show Material materials with Elongación of 17.2 % | Predicted Value, A200 | ||||
17.5 % Show Material materials with Elongación of 17.5 % | Predicted Value, A80 | |||||
19.3 % Show Material materials with Elongación of 19.3 % | Predicted Value, A80 Transverse | |||||
20.1 % Show Material materials with Elongación of 20.1 % | Predicted Value, A5 | |||||
20.9 % Show Material materials with Elongación of 20.9 % | Predicted Value, Transverse | |||||
23.2 % Show Material materials with Elongación of 23.2 % | Predicted Value, A50 | |||||
20 °C | 19 % Show Material materials with Elongación of 19 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Estricción | 42.7 % Show Material materials with Estricción of 42.7 % | Predicted Value | ||||
44.7 % Show Material materials with Estricción of 44.7 % | Predicted Value, Transverse | |||||
Límite elástico | 251.3 MPa Show Material materials with Límite elástico of 251.3 MPa | Predicted Value, RP1 | ||||
318.7 MPa Show Material materials with Límite elástico of 318.7 MPa | Predicted Value, RP1 Transverse | |||||
421.1 MPa Show Material materials with Límite elástico of 421.1 MPa | Predicted Value, RP02 | |||||
428.9 MPa Show Material materials with Límite elástico of 428.9 MPa | Predicted Value, Transverse | |||||
476.2 MPa Show Material materials with Límite elástico of 476.2 MPa | Predicted Value, RP02 Transverse | |||||
485.4 MPa Show Material materials with Límite elástico of 485.4 MPa | Predicted Value, RP002 | |||||
501.4 MPa Show Material materials with Límite elástico of 501.4 MPa | Predicted Value, RP05 | |||||
20 °C | 365 MPa Show Material materials with Límite elástico of 365 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 370 MPa Show Material materials with Límite elástico of 370 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 380 MPa Show Material materials with Límite elástico of 380 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 390 MPa Show Material materials with Límite elástico of 390 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 400 MPa Show Material materials with Límite elástico of 400 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 420 MPa Show Material materials with Límite elástico of 420 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
Módulo de cizallamiento | 80.2 GPa Show Material materials with Módulo de cizallamiento of 80.2 GPa | Predicted Value | ||||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | ||||
Resistencia a la tracción | 20 °C | 460 - 680 MPa Show Material materials with Resistencia a la tracción of 460 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
20 °C | 460 - 660 MPa Show Material materials with Resistencia a la tracción of 460 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 460 - 650 MPa Show Material materials with Resistencia a la tracción of 460 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 460 - 630 MPa Show Material materials with Resistencia a la tracción of 460 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 460 - 620 MPa Show Material materials with Resistencia a la tracción of 460 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 680 MPa Show Material materials with Resistencia a la tracción of 470 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 660 MPa Show Material materials with Resistencia a la tracción of 470 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 650 MPa Show Material materials with Resistencia a la tracción of 470 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 630 MPa Show Material materials with Resistencia a la tracción of 470 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 470 - 620 MPa Show Material materials with Resistencia a la tracción of 470 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 680 MPa Show Material materials with Resistencia a la tracción of 480 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 660 MPa Show Material materials with Resistencia a la tracción of 480 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 650 MPa Show Material materials with Resistencia a la tracción of 480 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 630 MPa Show Material materials with Resistencia a la tracción of 480 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 480 - 620 MPa Show Material materials with Resistencia a la tracción of 480 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 660 MPa Show Material materials with Resistencia a la tracción of 500 - 660 MPa | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire | ||
20 °C | 500 - 680 MPa Show Material materials with Resistencia a la tracción of 500 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 650 MPa Show Material materials with Resistencia a la tracción of 500 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 630 MPa Show Material materials with Resistencia a la tracción of 500 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 500 - 620 MPa Show Material materials with Resistencia a la tracción of 500 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 680 MPa Show Material materials with Resistencia a la tracción of 520 - 680 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 660 MPa Show Material materials with Resistencia a la tracción of 520 - 660 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 650 MPa Show Material materials with Resistencia a la tracción of 520 - 650 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 630 MPa Show Material materials with Resistencia a la tracción of 520 - 630 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
20 °C | 520 - 620 MPa Show Material materials with Resistencia a la tracción of 520 - 620 MPa | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | ||
Resistencia al cizallamiento | 532.5 MPa Show Material materials with Resistencia al cizallamiento of 532.5 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 455.2 J/(kg·K) Show Material materials with Calor específico of 455.2 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.86 1/K Show Material materials with Coeficiente de dilatación térmica of 11.86 1/K | Predicted Value |
Conductividad térmica | 38.04 W/(m·K) Show Material materials with Conductividad térmica of 38.04 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.025 % Show Material materials with Azufre of 0.025 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Carbono | 0.16 % Show Material materials with Carbono of 0.16 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Cobre | 0.55 % Show Material materials with Cobre of 0.55 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire |
0.03 % Show Material materials with Fósforo of 0.03 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar | |
Manganeso | 1.7 % Show Material materials with Manganeso of 1.7 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Molibdeno | 0.2 % Show Material materials with Molibdeno of 0.2 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Niobio | 0.05 % Show Material materials with Niobio of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar |
0.025 % Show Material materials with Nitrógeno of 0.025 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar |
0.8 % Show Material materials with Níquel of 0.8 % | thermomechanically rolled | EN 10025-4, EN 10113-3 | Strip, Sheet, Flat, Rod, Wire | |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Titanio | 0.05 % Show Material materials with Titanio of 0.05 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Vanadio | 0.12 % Show Material materials with Vanadio of 0.12 % | thermomechanically rolled | EN 10113-3, EN 10025-4 | Sheet, Strip, Bar, Flat, Rod, Wire |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |